2-Inch P-Type Silicon Wafer 0.01-0.1 Ω·cm DSP ATOMFAIR®

$359.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 2-inch (50.8 mm) P-type CZ silicon wafer, Boron-doped 0.01–0.1 Ω·cm, 275 ± 25 μm, DSP Ra < 0.5 nm. 25 pcs cassette. Order now.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•0.01–0.1 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 50.8 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat None (SEMI M1 standard for 50.8 mm P-type <111>) SEMI M1 (50.8 mm P<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 0.01-0.1 ohm-cm, 275 um, DSP (This Product) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type (0.01–0.1 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon substrates require particulate-controlled storage and edge-only manipulation to preserve sub-nanometer CMP surface quality. Ambient native oxide growth and moisture exposure must be managed prior to epitaxy, metallization, or thermal oxidation.

  • Cleanroom Storage Atmosphere: Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and contamination of the mirror-polished faces.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxy.
  • Wet-Chemical Processing Containment: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety guidelines.
  • Organic Contamination Control: Minimize airborne organic contamination by keeping unused wafers sealed in the original cassette box when not actively processed.

Sequential solvent cleaning, plasma descum, and native oxide management are required to preserve CMP surface quality and reproducible thin-film interfaces. All wet processing must follow institutional EHS and SDS safety protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect cassette and wafer edges
    Inspect the 25-wafer cleanroom cassette and wafer perimeter edges for particulate contamination or physical damage before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease sequentially in solvents
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood or wet bench.
  4. Dry with nitrogen
    Blow-dry the wafer with filtered N2 gas to remove residual solvent and water from both mirror-polished surfaces.
  5. Apply mild O2 plasma descum
    Apply a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide if required
    Perform RCA standard clean or wet oxide removal inside an exhaust fume hood or wet bench when native oxide removal is required before metallization or epitaxy.
  7. Return unused wafers to storage
    Return unused wafers to the original polypropylene cassette box and store sealed within a dry nitrogen cabinet or cleanroom desiccator.

Why choose a <111> P-type silicon wafer with 0.01–0.1 Ω·cm resistivity instead of a standard <100> wafer for epitaxy or device prototyping?

The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies, while the 0.01–0.1 Ω·cm boron doping lowers bulk series resistance for vertical current conduction and electrochemical electrodes. Compared with <100> silicon, the <111> plane also exhibits slower wet alkaline etch kinetics and higher in-plane elastic modulus along key cleavage directions. However, this low-resistivity P+ range reduces free-carrier infrared absorption relative to degenerately doped P++ substrates, making it suitable for IR transmission and anodic bonding.

Can this 2-inch DSP silicon wafer be used directly for double-side lithography and wafer bonding without additional surface preparation?

Yes, the dual-side mirror-polished (DSP) CMP finish with Ra < 0.5 nm is designed for double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The bare prime silicon surface carries only a thin ambient native oxide (~1–2 nm), so it can be processed directly in-house for thermal oxidation, wet etching, or epitaxial growth. For critical bonding or metallization steps, standard solvent pre-cleaning (acetone, IPA, DI water) followed by mild O2 plasma descum is recommended to preserve interface quality.

What are the storage and handling requirements to maintain the CMP surface quality of these prime-grade 2-inch silicon wafers?

Wafers must be stored sealed inside the original 25-wafer polypropylene cleanroom cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and contamination. The cassette is engineered to immobilize 2-inch wafer edges during transit, and each shipment includes a lot-specific Certificate of Analysis (CoA) documenting resistivity, thickness, orientation, and surface inspection criteria.

The 2-inch P-type <111> DSP silicon wafer with 0.01–0.1 Ω·cm resistivity offers a low-resistivity, double-side polished substrate suited for III-nitride epitaxy, wafer bonding, and electrochemical electrode prototyping. Its prime-grade virgin construction and SEMI M1 dimensional precision support reproducible 2-inch R&D processing, though the narrow resistivity window and <111> orientation constrain use to applications where these specific electrical and crystallographic properties are required.

Positive

  • Low-resistivity P+ bulk conduction: Boron doping to 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier IR absorption compared with degenerately doped P++ substrates.
  • Dual-side CMP mirror finish: Double-side polished surfaces with Ra < 0.5 nm enable double-sided lithography, through-wafer infrared transmission, and direct fusion or anodic bonding with reproducible thin-film interfaces.

Trade-offs

  • Narrow resistivity window: The 0.01–0.1 Ω·cm specification is a decade-wide P+ range; applications requiring tightly controlled resistivity or higher-resistivity substrates must select alternate wafer grades.
  • Native oxide and cleanroom handling: Bare prime silicon forms a ~1–2 nm native SiO2 film in air and must be stored in a dry nitrogen cabinet and handled by perimeter edge with cleanroom tools; wet processing requires exhaust fume hood or wet bench and institutional EHS/SDS compliance.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)