| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•0.001–0.005 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 carrier concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | None (SEMI M1 standard for 50.8 mm P-type <111>) | SEMI M1 (50.8 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 0.001-0.005 ohm-cm, 275 um, SSP (This Product) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type (0.001–0.005 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom-compatible handling to preserve the CMP-polished surface and prevent particulate or organic contamination. Storage must be maintained in a dry nitrogen cabinet or cleanroom desiccator to minimize native oxide growth and airborne molecular contamination.
- Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms a native silicon dioxide layer of approximately 1–2 nm in ambient air, which must be removed via RCA standard clean or wet etching prior to metallization or epitaxial growth.
- Storage Atmosphere: Store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination and moisture-driven oxidation.
- Wet Processing Safety: All wet-chemical processing, including RCA cleans and native oxide removal, must be performed inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning of prime-grade silicon wafers are essential to preserve surface quality and ensure reproducible thin-film interfaces. The following steps outline the recommended sequence for degreasing, native oxide control, and cleanroom storage.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect wafer cassette
Inspect the sealed 25-wafer cleanroom cassette for any signs of damage or particulate ingress before opening. - Transfer wafers
Transfer wafers individually from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling only by the perimeter edge. - Degrease wafer surface
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water to remove organic contaminants. - Dry and descum
Blow-dry the wafer with nitrogen gas and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide
Perform RCA standard clean or wet etching inside an exhaust fume hood to remove the native silicon dioxide layer before metallization or epitaxy. - Store unused wafers
Return unused wafers to the original polypropylene cassette and store sealed inside a dry nitrogen cabinet or cleanroom desiccator.
What is the resistivity and dopant concentration of this 2-inch P-type <111> silicon wafer?
This wafer is degenerately Boron-doped to a resistivity of 0.001–0.005 Ω·cm (P++), corresponding to a carrier concentration of approximately 1019–1020 cm-3. The low resistivity provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and electrochemical electrodes. Resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.
Why choose a <111> crystal orientation over <100> for silicon wafer epitaxy?
The <111> orientation offers a densely packed hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics compared to <100> silicon. These properties make it ideal for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. This wafer is oriented to <111> ± 0.5° as verified by X-ray diffraction.
How should I store and handle this prime silicon wafer to maintain surface quality?
Store wafers sealed inside the original 25-wafer cleanroom cassette within a dry nitrogen cabinet or desiccator to prevent particulate and organic contamination. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; avoid touching the polished front surface. The wafer is supplied in a 25-wafer cassette (25BX) and carries a native oxide of ~1–2 nm that can be removed via standard RCA clean or thermal oxidation.
The 2-inch P-type <111> prime silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and SSP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts and hexagonal epitaxy, but its <111> orientation and bare surface demand orientation-specific process tuning and immediate native-oxide management.
Positive
- Degenerate doping enables ohmic contacts: Boron-doped to 0.001–0.005 Ω·cm (P++), providing metallic-like bulk conductivity for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and electrochemical electrodes.
- <111> lattice supports hexagonal epitaxy: The densely packed <111> (± 0.5°) plane with three-fold symmetry and slower alkaline etch kinetics is suited for III-nitride (GaN, AlN, SiC) heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- <111> orientation requires process adaptation: The <111> crystal orientation exhibits slower wet alkaline etch kinetics than <100> silicon, necessitating orientation-specific etch recipes and potentially longer process times.
- Native oxide demands controlled removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film; removal before metallization or epitaxy requires wet processing in an exhaust fume hood or wet bench under institutional EHS protocols.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).