2-Inch N-Type Silicon Wafer 275μm SSP ATOMFAIR®

$259.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 0.01–0.1 Ω·cm, 275 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•0.01–0.1 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+), the wafer combines low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>) SEMI M1 (50.8 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (100), 0.01-0.1 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type (0.01–0.1 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers require cleanroom-compatible handling to preserve the CMP mirror surface and prevent particulate or organic contamination. Storage must minimize native oxide growth and airborne molecular contamination prior to processing.

  • Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA clean or wet processing before metallization or epitaxy.
  • Storage Atmosphere: Store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols inside an exhaust fume hood or wet bench.

Proper pre-cleaning and handling preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent degreasing followed by plasma descum removes organic contamination prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect wafer cassette
    Inspect the sealed 25-wafer cleanroom cassette for integrity and verify the lot-specific Certificate of Analysis before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic surface contamination.
  4. Blow-dry with nitrogen
    Blow-dry the wafer with filtered N2 to remove residual solvent and water before further processing.
  5. Perform plasma descum
    Perform a mild O2 plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide if required
    Remove the ambient 1–2 nm native SiO2 film via RCA standard clean or wet processing inside an exhaust fume hood when metallization or epitaxy is required.
  7. Store unused wafers
    Store unused wafers sealed inside the original polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.

What is the resistivity range of this 2-inch N-type silicon wafer and how does it affect device performance?

This wafer is Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm (N+), measured by four-point probe. This low-resistivity range provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, making it suitable for vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Is this wafer compatible with KOH or TMAH anisotropic wet etching for MEMS fabrication?

Yes. The wafer is sliced along the <100> crystal plane (± 0.5°), which supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions. The cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, and the primary flat is oriented along <110> ± 1° per SEMI M1 standards for accurate mask alignment.

How should these prime silicon wafers be stored and handled to preserve surface quality?

Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The CMP-polished front surface has Ra < 0.5 nm; bare prime silicon carries only a thin ambient native oxide (~1–2 nm) that can be removed via RCA clean or wet processing under facility-approved protocols.

The 2-inch N-type <100> prime silicon wafer with 0.01–0.1 Ω·cm phosphorus doping and SSP finish (Ra < 0.5 nm) is a well-characterized substrate for vertical diode prototyping, anisotropic KOH/TMAH micromachining, and calibration of thin-film processes in research-scale 2-inch chambers. Its low-resistivity N+ bulk reduces contact resistance while avoiding the free-carrier optical loss of degenerate doping, though the bare surface requires strict cleanroom handling and immediate pre-clean before critical deposition steps.

Positive

  • Low-resistivity N+ bulk for ohmic contacts: Phosphorus doping at 0.01–0.1 Ω·cm provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication and electrochemical electrode prototyping.
  • CMP mirror surface for uniform nucleation: Single-side polished front with Ra < 0.5 nm ensures reproducible thin-film growth and high-resolution photoresist spin coating for PVD, ALD, and e-beam evaporation processes.

Trade-offs

  • Native oxide requires pre-clean: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; removal via RCA clean or wet etch must be performed in an exhaust fume hood or wet bench following institutional EHS protocols before metallization or epitaxy.
  • Cleanroom storage and handling mandatory: Wafers must be stored sealed in the original cassette within a dry nitrogen cabinet or desiccator and handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)