| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.001–0.005 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers very low bulk series resistance for low-resistance backside ohmic contacts, conductive bottom electrodes, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>) | SEMI M1 (50.8 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (100), 0.001-0.005 ohm-cm, 275 um, DSP (This Product) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or desiccator to minimize native oxide growth and organic contamination.
- Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and contamination.
- Storage Environment: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning and plasma descum are required before photoresist spin coating or deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system
- Inspect wafer cassette
Inspect the sealed 25-wafer cleanroom cassette for integrity and verify the lot-specific Certificate of Analysis before opening. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. - Degrease sequentially
Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water. - Blow-dry with nitrogen
Blow-dry the wafer with N2 to remove residual solvents and moisture. - Perform plasma descum
Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove native oxide or perform RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when required before metallization or epitaxy. - Store unused wafers
Store unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity range of this 2-inch N-type silicon wafer and why does it matter for ohmic contacts?
This wafer is degenerately Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm (N++), corresponding to approximately 10^19–10^20 cm^-3 electron density. This very low bulk series resistance is specifically engineered for low-resistance backside ohmic contacts, conductive bottom electrodes, and high-current device testing. The tight resistivity window is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this double-side polished 2-inch wafer be used for KOH anisotropic etching and wafer bonding?
Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE). The dual-side CMP mirror finish (DSP, Ra < 0.5 nm) enables direct fusion and anodic bonding as well as double-sided MEMS patterning. The 50.8 ± 0.2 mm diameter and SEMI M1 flats ensure accurate registration on vacuum chucks and mask aligners.
How should these prime silicon wafers be stored and handled to preserve the CMP surface?
Wafers are supplied in a standard 25-wafer cleanroom cassette (25BX) that immobilizes edges and prevents surface contact. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any wet processing must follow institutional EHS and SDS protocols.
This 2-inch prime CZ N-type silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with dual-side CMP polishing (Ra < 0.5 nm) and SEMI M1 geometry, making it well-suited for low-resistance ohmic contact prototyping, double-side lithography, and anisotropic KOH/TMAH micromachining in research-scale chambers. Its bare, uncoated surface and 275 μm thickness demand careful native-oxide management and edge-only cleanroom handling to preserve the polished interface.
Positive
- Degenerate N++ Doping for Ohmic Contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), the wafer provides very low bulk series resistance for backside ohmic contacts, conductive bottom electrodes, and high-current device testing.
- Dual-Side CMP for Bonding and Lithography: Double-side mirror polish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding with reproducible thin-film growth.
Trade-offs
- Native Oxide Requires Pre-Clean: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal via RCA or wet processing must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols before metallization or epitaxy.
- Edge-Only Cleanroom Handling Required: The CMP mirror surface is vulnerable to particulate and organic contamination; wafers must be handled strictly by the perimeter edge with vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).