| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.01–0.1 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+), the wafer combines low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>) | SEMI M1 (50.8 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (100), 0.01-0.1 ohm-cm, 275 um, DSP (This Product) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, N-Type (0.01–0.1 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon substrates require particulate-controlled storage and edge-only manipulation to preserve CMP surface quality. Ambient native oxide growth and atmospheric contamination must be managed prior to any thin-film, lithographic, or bonding process.
- Cleanroom Storage Atmosphere: Store unused wafers sealed in the original polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the mirror-polished CMP surfaces.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA standard clean or wet processing before metallization or epitaxy.
- Wet-Chemical Processing Containment: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
- Cassette Immobilization: The 25-wafer cleanroom cassette immobilizes wafer edges to prevent surface contact during transit and must remain sealed until the wafers are introduced into the process environment.
Sequential solvent degreasing followed by plasma descum removes organic contamination from CMP surfaces prior to resist coating or vacuum deposition. Native oxide removal is performed under exhaust ventilation when ohmic or epitaxial interfaces are required.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet
- Transfer wafer from cassette
Transfer the wafer from its sealed cleanroom cassette using a vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic surface contamination. - Dry with nitrogen
Blow-dry the wafer with filtered N2 until all visible solvent and water residue is removed from both polished faces. - Apply plasma descum
Apply a mild O2 plasma descum to eliminate residual organics prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide under ventilation
Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS/SDS controls. - Return unused wafers to storage
Return unused wafers to the original polypropylene cassette and store sealed within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity range of this 2-inch N-type silicon wafer, and how does it affect device fabrication?
This wafer is Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm (N+), measured by four-point probe. This low-resistivity range provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, making it suitable for vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.
Can this 2-inch DSP wafer be used for double-side lithography and wafer bonding processes?
Yes. The wafer features dual-side mirror-polished surfaces (DSP) with a CMP finish achieving Ra < 0.5 nm, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The <100> crystal orientation with SEMI M1 flats ensures accurate registration on vacuum chucks and mask aligners.
How should these prime-grade silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in a standard 25-wafer cleanroom cassette (25BX) designed to immobilize edges and prevent surface contact during transit.
This 2-inch prime CZ N-type silicon wafer combines a low-resistivity phosphorus-doped substrate (0.01–0.1 Ω·cm) with dual-side CMP polishing (Ra < 0.5 nm) and SEMI M1 dimensional precision, making it well-suited for double-side lithography, MEMS micromachining, and electrochemical electrode prototyping. However, its bare prime surface requires strict cleanroom handling and immediate native-oxide management to preserve interface quality.
Positive
- Low-Resistivity N+ Substrate: Phosphorus doping at 0.01–0.1 Ω·cm provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication and electrochemical electrodes.
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm enable reproducible thin-film growth, double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet processing for native oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
- Strict Cleanroom Storage Needed: To prevent particulate and organic contamination, unused wafers must remain sealed in the original 25-wafer cassette within a dry nitrogen cabinet or cleanroom desiccator, and handled only by edge with vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).