Prime CZ N-Type silicon wafer, 125mm, 625μm, 100–1000 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats. In stock.

Diameter & Flat:
5-Inch (125.0 ± 0.5 mm)
Primary Flat 42.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•100–1000 Ω·cm
Thickness:
625 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar waveguides, IR/THz transmission windows (especially DSP), radiation/particle detector prototyping, and MEMS sensor isolation.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 5-Inch Dimensional Precision

Standardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 125.0 ± 0.5 mm (5.0 Inch)
  • Primary Flat: 42.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 27.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 125 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 125.0 ± 0.5 mm (5-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 625 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 42.5 ± 2.5 mm SEMI M1 (125 mm)
Secondary Flat 27.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 125 mm N<111>) SEMI M1 (125 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 5-Inch (125 mm), N-Type (111), 100-1000 ohm-cm, 625 um, SSP (This Product) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <100> Standard SEMI M1 625 μm 125 mm P-type lithography substrate
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) 5-Inch (125 mm) / DSP 625 ± 25 μm, P-Type <100> Double-side CMP polished 125 mm wafer for IR optics & bonding
5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type <100> Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D
5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <111> Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve sub-nanometer surface quality and prevent particulate contamination. Storage must occur in a dry nitrogen environment to minimize native oxide growth and airborne organic deposition.

  • Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contact with the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing inside an exhaust fume hood or wet bench when native oxide removal is necessary.
  • Storage Atmosphere: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Particulate and Vapor Exposure: Keep wafers away from particulate dust and corrosive vapors to maintain surface particle counts at or below 10 particles per wafer.

Proper handling and pre-cleaning of prime silicon wafers preserves CMP surface quality and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet

  1. Inspect cassette packaging
    Verify the cleanroom protective cassette is intact and the wafer edges are immobilized without surface contact before opening.
  2. Transfer wafer by edge
    Handle the wafer strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and descum
    Blow-dry with N2 and perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide under hood
    Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  6. Store unused wafers sealed
    Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

Why choose a high-resistivity 100–1000 Ω·cm N-type <111> silicon wafer instead of a standard 1–10 Ω·cm substrate?

The 100–1000 Ω·cm Phosphorus-doped bulk suppresses conductive substrate coupling and parasitic RF loss, which is critical for RF/microwave planar waveguides, IR/THz transmission windows, and radiation detector prototyping. Standard 1–10 Ω·cm wafers are optimized for CMOS and power R&D, but their lower resistivity introduces higher dielectric loss and substrate leakage at high frequency. This wafer is therefore specified where substrate isolation, not carrier concentration, dominates device performance.

Can this 5-inch <111> SSP wafer be used directly for GaN, AlN, or SiC epitaxy without an additional buffer layer?

The <111> (± 0.5°) orientation provides the hexagonal three-fold surface symmetry required for lattice-matched III-nitride and SiC heteroepitaxy, and the SSP front surface with Ra < 0.5 nm supports uniform nucleation. However, the wafer is supplied as bare prime silicon with only a ~1–2 nm ambient native oxide and no epitaxial-ready coating, so standard ex-situ HF or RCA cleaning and typically a nucleation or buffer layer are still required before growth. It is not a pre-epi wafer.

What cleanroom handling and storage conditions are required to preserve the SSP Ra < 0.5 nm surface before processing?

Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and unused wafers should remain sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or desiccator away from particulates and corrosive vapors. The CMP finish is verified at ≤ 10 particles per wafer, so any airborne organic or particulate exposure before lithography or ALD will degrade the Ra < 0.5 nm interface. All wet-chemical cleaning must follow institutional EHS and SDS protocols.

The 5-inch N-type <111> prime CZ silicon wafer with 100–1000 Ω·cm resistivity and SSP finish offers a high-resistivity, crystallographically oriented substrate suited for RF/microwave planar waveguides, hexagonal epitaxy, and detector prototyping. Its SEMI M1 geometry and 625 μm thickness ensure compatibility with standard cleanroom cassettes and vacuum chucks, though handling requires strict edge-only protocols and dry storage to preserve the sub-nanometer surface finish.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this wafer suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar waveguides and IR/THz transmission windows.
  • <111> Orientation for Hexagonal Epitaxy: The <111> crystal plane provides three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in air; wet processing to remove it must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
  • Strict Cleanroom Handling Required: To preserve the Ra < 0.5 nm CMP surface, wafers must be handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers and stored in a dry nitrogen cabinet or desiccator.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

5-Inch (125.0 ± 0.5 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

625 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)