4-Inch Prime Silicon Wafer P-Type 525μm DSP ATOMFAIR®

Price range: $229.00 through $489.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type/Boron 4-inch wafer, 20–50 Ω·cm, 525 ± 25 μm, DSP Ra < 0.5 nm, SEMI M1 flats. In stock in 10/25 pcs cassettes.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•20–50 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 20–50 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Boron-doped to 20–50 Ω·cm (~3×1014–7×1014 cm-3 hole concentration), this low-doping substrate widens depletion layers and lowers junction capacitance for optical/particle photodetectors, PIN photodiodes, and low-noise analog test structures.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 100 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 20–50 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat None (SEMI M1 standard for 100 mm P-type <111>) SEMI M1 (100 mm P<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (20–50 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 20-50 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type (20–50 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage to prevent particulate contamination and native oxide growth. Handling must avoid surface contact and exposure to corrosive vapors that degrade the CMP finish.

  • Cleanroom Storage Environment: Store wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished surfaces.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed via RCA clean or wet etching before metallization or epitaxy if an oxide-free interface is required.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, and native oxide removal must be performed inside an exhaust fume hood or wet bench.

Proper handling and pre-cleaning procedures preserve the CMP surface quality and ensure reproducible thin-film interfaces. These steps cover degreasing, native oxide control, and safe storage of prime silicon wafers.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or desiccator

  1. Inspect wafer cassette
    Inspect the cleanroom cassette for any particulate contamination or damage before opening.
  2. Handle wafer by edge
    Handle the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease wafer surface
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water.
  4. Dry with nitrogen
    Blow-dry the wafer with filtered nitrogen gas until all visible liquid is removed.
  5. Perform plasma descum
    Perform a mild oxygen plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD.
  6. Remove native oxide if required
    Remove the native oxide via RCA standard clean or wet etching inside an exhaust fume hood or wet bench if an oxide-free interface is required.
  7. Store unused wafers properly
    Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> orientation P-type silicon wafer with 20–50 Ω·cm resistivity over a standard <100> wafer?

The <111> orientation provides a hexagonal three-fold surface symmetry and higher in-plane elastic modulus along key cleavage directions, which supports III-nitride/hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies. The 20–50 Ω·cm boron doping widens depletion layers and lowers junction capacitance, making it suitable for optical/particle photodetectors, PIN photodiodes, and low-noise analog test structures. Additionally, <111> silicon exhibits slower wet alkaline etch kinetics than <100>, which can be advantageous for certain etching processes.

Can this 4-inch DSP wafer be used for double-side lithography and wafer bonding?

Yes, the dual-side mirror-polished surfaces (DSP, Ra < 0.5 nm) enable double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding. The 525 ± 25 μm thickness provides high flexural rigidity for handling in automated equipment. The wafer is prime-grade virgin silicon with no coating, allowing direct in-house thermal oxidation or epitaxial growth.

What are the storage and handling requirements to maintain the surface quality of these prime silicon wafers?

Wafers should be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.

The 4-inch P-type <111> DSP silicon wafer combines a low-doping 20–50 Ω·cm bulk with dual-side CMP finish (Ra < 0.5 nm) and SEMI M1 geometry, making it well suited to hexagonal epitaxy, double-side lithography, and low-noise device prototyping. Its main operational constraints are the need for cleanroom edge handling and wet-bench processing to preserve the bare, native-oxide-bearing surfaces.

Positive

  • Low-doping bulk for wide depletion: Boron doping at 20–50 Ω·cm (~3×10^14–7×10^14 cm^-3) widens depletion layers and lowers junction capacitance, supporting PIN photodiodes, optical/particle detectors, and low-noise analog test structures.
  • Dual-side CMP for bonding and IR: DSP finish with Ra < 0.5 nm on both faces enables double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding without additional surface preparation.

Trade-offs

  • Bare surface requires cleanroom handling: Uncoated prime silicon carries only a 1–2 nm native oxide and must be handled by the perimeter edge with vacuum wands or PTFE/PEEK tweezers; storage in a dry nitrogen cabinet or cleanroom desiccator is required to avoid particulate and organic contamination.
  • Wet processing needs fume-hood infrastructure: Native oxide removal and RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols, adding facility and safety infrastructure requirements to the process flow.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

20-50 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)