| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•1–10 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | None (SEMI M1 standard for 100 mm P-type <111>) | SEMI M1 (100 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 1-10 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (1–10 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm, 380 μm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Intermediate 76.2 mm wafer for compact research chambers |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon forms a native oxide layer in ambient air and is sensitive to particulate, organic, and metallic contamination. Storage must occur in a dry nitrogen cabinet or cleanroom desiccator to preserve surface quality.
- Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1–2 nm in air, which must be removed before metallization or epitaxy if an oxide-free interface is required.
- Particulate and Organic Contamination Control: Wafers must be stored sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination and particulate deposition.
- Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and contamination of the polished face.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, with native oxide removal or RCA standard clean performed inside an exhaust fume hood or wet bench.
Proper handling and pre-cleaning preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the wafer for photoresist spin coating or PVD/ALD deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect wafer packaging
Inspect the cleanroom protective cassette for seal integrity and verify the lot-specific Certificate of Analysis against the required resistivity, thickness, and orientation specifications. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling strictly by the perimeter edge to avoid contact with the polished surface. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water to remove organic contaminants from the CMP surface. - Dry with nitrogen
Blow-dry the wafer with filtered nitrogen gas to remove residual solvent and water without leaving streaks or particles. - Apply mild O2 plasma descum
Apply a mild oxygen plasma descum to remove residual organic species prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when an oxide-free interface is required before metallization or epitaxy. - Store unused wafers sealed
Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a <111> oriented silicon wafer over <100> for epitaxy or surface science?
The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies, unlike <100> silicon. It also exhibits a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100>, making it preferable for hexagonal epitaxy and discrete power/bipolar R&D. This wafer is specified to <111> ± 0.5° per XRD, ensuring consistent surface registry.
Can this 4-inch P-type <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?
Yes, the wafer is bare prime silicon with only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial growth. However, for reproducible interfaces, the source recommends solvent pre-cleaning (acetone, IPA, DI water) and mild O2 plasma descum before photoresist spin coating or PVD/ALD. For native oxide removal or RCA clean prior to metallization, perform wet processing in an exhaust fume hood using facility-approved protocols.
What are the storage and handling requirements to maintain the Ra < 0.5 nm surface of this SSP wafer?
Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particulate dust. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. The wafer is supplied in cleanroom protective cassettes (10 pcs or 25 pcs) that immobilize edges and prevent surface contact during transit.
The 4-inch P-type <111> prime CZ silicon wafer offers a well-characterized 1–10 Ω·cm boron-doped substrate with a sub-nanometer CMP finish and SEMI M1 dimensional precision, making it a reliable platform for hexagonal epitaxy, device prototyping, and thin-film metrology. Its 525 μm thickness and SSP/ground-back configuration impose careful handling and cleaning requirements, but the lot-specific CoA and virgin prime-grade provenance support reproducible cleanroom integration.
Positive
- Sub-nanometer CMP surface finish: The single-side polished front surface with Ra < 0.5 nm provides uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating, supporting reproducible thin-film growth and lithography.
- Dense <111> lattice for hexagonal epitaxy: The <111> ± 0.5° crystal orientation offers three-fold surface symmetry and slower wet alkaline etch kinetics, enabling lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- Native oxide requires pre-clean control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, so native oxide removal or RCA cleaning must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols before metallization or epitaxy.
- Edge-only handling and dry storage: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or cleanroom desiccator to prevent particulate and organic contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.