| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•0.1–1.0 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 0.1–1.0 Ω·cm (~2×1016–2×1017 cm-3 acceptor concentration), this moderately low-resistivity substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.1–1.0 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | None (SEMI M1 standard for 100 mm P-type <111>) | SEMI M1 (100 mm P<111>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.1–1.0 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 0.1-1.0 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type (0.1–1.0 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in sealed cleanroom cassettes within dry nitrogen cabinets or desiccators away from dust and corrosive vapors.
- Surface Contamination Sensitivity: The dual-side mirror-polished CMP surface with Ra < 0.5 nm is highly susceptible to particulate contamination and organic adsorption, requiring strict cleanroom protocols during all handling operations.
- Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide layer of approximately 1–2 nm in air, which must be removed via wet processing or RCA standard clean before metallization or epitaxial growth.
- Mechanical Fragility: The 525 ± 25 μm thickness wafer requires edge-only handling with vacuum wands or PTFE/PEEK tweezers to prevent surface scratches and fracture.
- Environmental Storage Requirements: Unused wafers must remain sealed inside original cleanroom polypropylene cassette boxes within dry nitrogen cabinets to minimize airborne organic contamination and moisture exposure.
Proper handling preserves the CMP surface quality and ensures reproducible thin-film interfaces for semiconductor processing. Sequential solvent cleaning and controlled storage prevent contamination that degrades device performance.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Verify the cleanroom protective cassette is intact and the wafer edges are properly immobilized before opening. - Transfer wafer by edge
Handle the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid surface contact. - Perform solvent pre-cleaning
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water followed by nitrogen blow-drying. - Apply plasma descum
Subject the cleaned wafer to mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when native oxide removal or RCA standard clean is necessary. - Store unused wafers properly
Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet.
Why choose a <111> orientation P-type silicon wafer over <100> for epitaxy or power device prototyping?
The <111> orientation provides a densely packed three-fold surface symmetry with a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. This makes it preferable for lattice-matched III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete bipolar/power R&D. The <100> orientation is generally favored for standard CMOS lithography and MEMS DRIE, so the choice depends on whether your process requires hexagonal symmetry or standard planar integration.
Can this 4-inch DSP wafer be used for double-side lithography and wafer bonding?
Yes. The dual-side CMP mirror finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 525 ± 25 μm thickness provides high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Note that the wafer is bare prime silicon with only a thin ambient native oxide (~1–2 nm), so any native oxide removal or RCA clean must be performed before metallization or epitaxy.
What are the storage and handling requirements to preserve the CMP surface of this prime silicon wafer?
Store wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. The wafers ship in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize 4-inch wafer edges during transit, and each shipment includes a lot-specific Certificate of Analysis documenting resistivity, thickness, orientation, and surface inspection criteria.
The 4-inch P-type <111> prime silicon wafer with 0.1–1.0 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a well-characterized substrate for hexagonal epitaxy, double-side lithography, and UHV surface studies. Its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling, though the <111> orientation and moderate doping require process adjustments compared to conventional <100> CMOS wafers.
Positive
- Dual-Side CMP for Bonding and Lithography: Double-side mirror-polished surfaces (DSP, Ra < 0.5 nm) enable direct fusion/anodic bonding, through-wafer IR transmission, and double-sided MEMS patterning with sub-nanometer roughness.
- <111> Orientation for Hexagonal Epitaxy: The densely packed <111> crystal plane provides three-fold surface symmetry and slower alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure ohmic interfaces.
- <111> Orientation Limits CMOS Compatibility: The <111> crystal orientation is not standard for mainstream CMOS processing, requiring process redevelopment for lithography, etching, and dopant activation compared to <100> wafers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).