4-Inch Prime Silicon Wafer P-Type 525 μm ATOMFAIR®

Price range: $169.00 through $349.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type/Boron silicon wafer, 100.0 ± 0.3 mm, 525 ± 25 μm, 0.1–1.0 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•0.1–1.0 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Boron-doped to 0.1–1.0 Ω·cm (~2×1016–2×1017 cm-3 acceptor concentration), this moderately low-resistivity substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 100 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.1–1.0 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat None (SEMI M1 standard for 100 mm P-type <111>) SEMI M1 (100 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.1–1.0 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 0.1-1.0 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type (0.1–1.0 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve the CMP-polished surface and prevent particulate contamination. Environmental exposure to airborne organics, corrosive vapors, and uncontrolled humidity must be minimized to maintain sub-nanometer surface roughness and native oxide reproducibility.

  • Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy where oxide removal is critical.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.

Proper pre-cleaning and handling preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces across cleanroom processing runs. Sequential solvent degreasing followed by plasma descum and controlled storage minimizes organic and particulate contamination.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system

  1. Inspect wafer cassette
    Inspect the cleanroom cassette for edge damage or particulate contamination before removing any wafer.
  2. Transfer wafer by edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease sequentially
    Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water.
  4. Blow-dry with nitrogen
    Blow-dry the wafer with filtered nitrogen gas to remove residual solvent.
  5. Apply mild O2 plasma descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Return unused wafers to storage
    Return unused wafers to the sealed cleanroom cassette within a dry nitrogen cabinet.

Why choose a <111> orientation silicon wafer over <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed crystal plane with hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon. These properties make it preferable for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. In contrast, <100> wafers are typically chosen for standard CMOS lithography and MEMS DRIE due to their faster etch rates and different surface chemistry.

What are the storage and handling requirements for prime-grade silicon wafers to maintain surface quality?

Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the polished surface. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.

Can this 4-inch P-type <111> wafer be used for thermal oxidation and what is the native oxide thickness?

Yes, bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth. The wafer is suitable for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration. For native oxide removal or RCA standard clean before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols.

The 4-inch P-type <111> prime CZ silicon wafer with 0.1–1.0 Ω·cm resistivity and SSP finish offers a lattice-matched platform for hexagonal epitaxy and power device prototyping, though its moderate resistivity and single-side polish impose constraints on high-frequency or double-side-processed applications.

Positive

  • Hexagonal Lattice for III-Nitride Epitaxy: The <111> crystal orientation provides three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
  • Sub-Nanometer CMP Surface Finish: Single-side polished front surface with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, and high-resolution photoresist spin coating, enabling reproducible thin-film growth and lithography.

Trade-offs

  • Moderate Resistivity Limits High-Frequency Use: Boron-doped to 0.1–1.0 Ω·cm, this substrate is unsuitable for RF or high-speed devices requiring lower resistivity; it is intended for epitaxial templates and power/bipolar R&D.
  • Single-Side Polish Restricts Double-Side Processes: The fine-ground back surface precludes fusion bonding or backside lithography; double-side polished (DSP) wafers are required for those applications.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.1-1.0 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)