| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•0.01–0.1 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic glass bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | None (SEMI M1 standard for 100 mm P-type <111>) | SEMI M1 (100 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 0.01-0.1 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (0.01–0.1 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulate contamination, corrosive vapors, and ambient moisture must be minimized during storage and processing.
- Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and contamination of the polished face.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy where oxide removal is critical.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.
Proper pre-cleaning and handling procedures preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the wafer surface for photoresist spin coating or thin-film deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer cassette
Verify the cleanroom protective cassette is sealed and the wafer edges are immobilized without surface contact before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water within an exhaust fume hood or wet bench. - Dry with nitrogen
Blow-dry the wafer surface with filtered N2 to remove residual solvent and water before further processing. - Perform plasma descum
Apply a mild O2 plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD deposition. - Return unused wafers to storage
Seal unused wafers inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a <111> orientation P-type silicon wafer with 0.01–0.1 Ω·cm resistivity instead of a standard <100> wafer?
The <111> orientation provides a densely packed three-fold surface symmetry with higher in-plane elastic modulus and slower wet alkaline etch kinetics than <100> silicon, making it preferable for III-nitride/hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies. The 0.01–0.1 Ω·cm boron-doped (P+) resistivity lowers bulk series resistance for vertical current conduction and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates. Standard <100> wafers remain the default for general lithography and MEMS, but <111> is specifically suited to hexagonal epitaxy and discrete power/bipolar R&D.
Can this 4-inch P-type <111> prime silicon wafer be used directly for thermal oxidation or epitaxial growth without additional surface preparation?
Yes, the wafer is a bare prime silicon substrate carrying only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth. The single-side polished front surface has a CMP finish with Ra < 0.5 nm, which supports uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating. For native oxide removal or RCA standard clean before metallization or epitaxy, wet processing must be performed strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
What are the storage and handling requirements to maintain the surface quality of these prime-grade 4-inch silicon wafers?
Wafers should be stored sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit.
This 4-inch prime CZ P-type <111> silicon wafer combines a low 0.01–0.1 Ω·cm boron-doped bulk with a sub-nanometer CMP front surface, making it well suited to hexagonal III-nitride epitaxy, electrochemical electrode prototyping, and in-house thermal oxidation. Its 525 μm SEMI M1 geometry and bare prime surface, however, require cleanroom cassette handling and prompt native-oxide management before any metallization or epitaxial step.
Positive
- Low-Resistivity P+ Bulk Conduction: Boron doping at 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction, anodic glass bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption relative to degenerately doped P++ substrates.
- <111> Lattice for Hexagonal Epitaxy: The <111> (± 0.5°) orientation offers three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
- CMP Mirror Surface for Thin Films: Single-side CMP polishing to Ra < 0.5 nm with ≤ 10 particles per wafer supports uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
- SEMI M1 Geometry and Rigidity: The 100.0 ± 0.3 mm diameter, 525 ± 25 μm thickness, TTV < 5 μm, and bow/warp < 30 μm provide high flexural rigidity compatible with steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; native oxide removal or RCA standard clean must be performed in an exhaust fume hood or wet bench under facility-approved protocols before metallization or epitaxy.
- Cleanroom Storage and Handling: Wafers must be stored sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors, and handled strictly by the perimeter edge using vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).