4-Inch Prime CZ Silicon Wafer P-Type DSP 525μm ATOMFAIR®

Price range: $209.00 through $459.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type/Boron silicon wafer, 100.0 ± 0.3 mm, 525 ± 25 μm, 1–10 Ω·cm, DSP Ra < 0.5 nm, SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•1–10 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 1-10 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type (1–10 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth
3-Inch P-Type <100> Wafer (1–10 Ω·cm, 380 μm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Intermediate 76.2 mm wafer for compact research chambers

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or desiccator to minimize native oxide growth and airborne organic contamination.

  • Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle transfer.
  • Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA clean or wet processing before metallization or epitaxy.
  • Storage Atmosphere: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning of prime silicon wafers preserve surface quality and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contaminants prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Inspect the cleanroom cassette for any particulate contamination or damage before opening.
  2. Handle wafer by edge
    Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Degrease wafer surface
    Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and descum
    Blow-dry with nitrogen and perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide if required
    Perform RCA standard clean or wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when native oxide removal is required.
  6. Store unused wafers
    Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

Can I use this 4-inch DSP wafer for KOH anisotropic etching and DRIE, and what crystal orientation constraints apply?

Yes. The wafer is a <100> (± 0.5°) CZ monocrystalline silicon substrate, which supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE). The primary flat is 32.5 ± 2.5 mm along <110> ± 1°, and the secondary flat is 18.0 ± 2.0 mm located 90° ± 5° clockwise from the primary flat per SEMI M1 100 mm P<100>, enabling accurate mask alignment for <110>-directed cleaving and etch features.

What is the native oxide thickness on this bare prime silicon wafer, and how should it be removed before metallization or epitaxy?

Bare prime silicon carries only a thin ambient native oxide of approximately 1–2 nm. For native oxide removal or RCA standard clean before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. The wafer has no deposited film or coating, so direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth is possible after appropriate surface preparation.

How should these 4-inch prime wafers be stored and handled to maintain CMP surface quality and low particle counts?

Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the dual-side mirror-polished surfaces (DSP, Ra < 0.5 nm). The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during transit, and each batch is inspected to ≤ 10 particles per wafer.

This 4-inch prime CZ P-type <100> silicon wafer combines a dual-side CMP finish (Ra < 0.5 nm) with SEMI M1 dimensional tolerances and a verified 1–10 Ω·cm boron-doped bulk, making it a well-characterized substrate for double-side lithography, anisotropic KOH/TMAH micromachining, and C-V or Schottky metrology. Its bare, uncoated surface and 525 μm thickness suit in-house thermal oxidation and thin-film growth, but deployment requires cleanroom cassette handling and wet-bench infrastructure to preserve the native-oxide and particle specifications.

Positive

  • Dual-Side CMP Mirror Finish: DSP surfaces with Ra < 0.5 nm support double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding where single-side-polished substrates cannot be used.
  • <100> Plane Enables Anisotropic Etch: The <100> (± 0.5°) orientation with <110> primary flat provides four-fold symmetry and predictable KOH/TMAH V-groove formation, with low Si/SiO2 interface state density for MOS prototyping.

Trade-offs

  • Native Oxide Requires Wet-Bench Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal or RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols.
  • Cleanroom Storage and Edge Handling: Unused wafers must remain sealed in the original polypropylene cassette within a dry nitrogen cabinet or desiccator, and handled only by perimeter edge with vacuum wands or PTFE/PEEK tweezers to avoid particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)