4-Inch Prime CZ Silicon Wafer P-Type 380μm DSP ATOMFAIR®

Price range: $259.00 through $569.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch (100 mm) CZ P-Type/Boron silicon wafer, 0.001–0.005 Ω·cm, 380 ± 25 μm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•0.001–0.005 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 380 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 carrier concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The thinned 380 ± 25 μm profile accelerates through-wafer DRIE/wet etching, enhances thermal transfer during rapid thermal processing (RTP), and increases mid/far-infrared optical transmission. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.001-0.005 ohm-cm, 380 um, DSP (This Product) 4-Inch (100 mm) / DSP 380 ± 25 μm, P-Type (0.001–0.005 Ω·cm) SEMI M1 380 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination that degrades lithographic and epitaxial interfaces. Storage and handling must preserve the CMP mirror finish and prevent crystal-plane damage prior to cleanroom processing.

  • Atmospheric Native Oxide Formation: Exposure to ambient air forms a ~1–2 nm native SiO2 film that must be removed by RCA clean or wet processing before metallization or epitaxy.
  • Particulate and Organic Contamination Control: Airborne organics and particles degrade the Ra < 0.5 nm CMP surface, requiring sealed cassette storage in a dry nitrogen cabinet or cleanroom desiccator.
  • Edge-Contact Handling Restriction: Direct surface contact causes scratches and contamination, so wafers must be handled strictly by the perimeter edge using vacuum wands or PTFE/PEEK tweezers.
  • Corrosive Vapor Exposure: Storage near corrosive vapors or particulate dust compromises surface quality and must be avoided to maintain batch-verified cleanliness.
  • Wet-Chemical Processing Safety: KOH, TMAH, RCA, and solvent-based cleans require exhaust fume hood or wet bench operation under institutional EHS and SDS protocols.

Preserve the dual-side CMP mirror finish and reproducible thin-film interfaces by following sequential solvent cleaning, plasma descum, and controlled storage. All wet-chemical steps must be performed under institutional EHS and SDS safety protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette box, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect cassette on receipt
    Verify the cleanroom protective cassette is sealed and the wafer edges are immobilized without surface contact before opening.
  2. Transfer wafer by edge
    Handle the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid surface contact.
  3. Degrease sequentially in solvents
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues.
  4. Dry and descum
    Blow-dry with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide where required
    Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench using facility-approved protocols before metallization or epitaxy.
  6. Store unused wafers sealed
    Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet to minimize airborne organic contamination.

What is the resistivity and carrier concentration of this 4-inch P-type boron-doped silicon wafer?

This wafer is degenerately Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm (P++), corresponding to a carrier concentration of approximately 10^19–10^20 cm^-3. The low resistivity provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and electrochemical electrodes. Resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.

Can this 380 µm thick DSP wafer be used for double-side lithography and wafer bonding?

Yes. The wafer features a dual-side mirror-polished (DSP) CMP finish with Ra < 0.5 nm on both surfaces, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 380 ± 25 µm thickness also enhances mid/far-infrared optical transmission and accelerates through-wafer DRIE or wet etching compared to standard 525 µm wafers.

How should these prime-grade silicon wafers be stored and handled to preserve surface quality?

Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm CMP surfaces. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers sealed until processing to minimize airborne organic contamination.

The 4-inch prime CZ P-type boron-doped silicon wafer (0.001–0.005 Ω·cm, 380 μm, DSP) delivers degenerate P++ conductivity and sub-nanometer CMP surfaces suited to low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and double-side lithography. Its thinned 380 μm profile accelerates through-wafer DRIE and wet etching while enhancing IR transmission, but the bare native oxide and tight flat tolerances impose strict cleanroom handling and pre-metallization oxide removal.

Positive

  • Degenerate P++ Bulk Conductivity: Boron-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), providing metallic-like bulk conductivity for low-resistance ohmic contacts, electrochemical electrodes, and high-power epitaxy.
  • Dual-Side CMP Mirror Finish: Double-side polished with Ra < 0.5 nm supports double-sided MEMS patterning, direct fusion/anodic bonding, and reproducible thin-film growth or lithography.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench before metallization or epitaxy.
  • Strict Cleanroom Handling Mandate: Wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)