| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.001–0.005 Ω·cm |
Thickness: 500 ± 15 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 500 ± 15 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 carrier concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The 500 ± 15 μm tight-tolerance thickness suits precision MEMS micromachining, double-side alignment lithography, DRIE through-etching, and reproducible capacitive cavity fabrication. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 500 ± 15 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.001-0.005 ohm-cm, 500 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 500 ± 15 μm, P-Type (0.001–0.005 Ω·cm) | SEMI M1 500 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom-compatible handling to preserve sub-nanometer surface quality. Storage must prevent particulate contamination, native oxide growth, and mechanical damage to the mirror-polished surfaces.
- Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Storage Atmosphere Control: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for oxide removal before metallization or epitaxy.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the wafer surface for photoresist coating or deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Inspect the cleanroom protective cassette for edge immobilization and absence of particulate contamination before opening. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. - Degrease sequentially
Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry with nitrogen
Dry the wafer surface with a nitrogen blow-dry immediately after the final DI water rinse. - Perform plasma descum
Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
What is the resistivity of this 4-inch P-type silicon wafer and how does it affect ohmic contact formation?
This wafer is Boron-doped to a resistivity of 0.001–0.005 Ω·cm (P++), corresponding to a carrier concentration of approximately 10^19–10^20 cm^-3. This degenerate doping level provides metallic-like bulk conductivity, which is specifically suitable for forming low-resistance ohmic contacts in device prototyping. The low resistivity also supports applications such as cryogenic back-gated 2D FETs and electrochemical electrodes.
Can this 500 µm thick DSP wafer be used for double-side alignment lithography and through-wafer etching?
Yes. The 500 ± 15 µm thickness and dual-side mirror-polished surfaces (DSP, Ra < 0.5 nm) are designed for double-side alignment lithography and DRIE through-etching. The tight thickness tolerance supports reproducible capacitive cavity fabrication and precision MEMS micromachining. The <100> crystal orientation enables anisotropic wet etching in KOH or TMAH solutions for V-groove formation.
How should these prime-grade silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed in the original cleanroom protective cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination. The wafers are shipped in cassettes that immobilize edges and prevent surface contact during transit.
The 4-inch prime CZ P-type <100> silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and dual-side CMP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts, MEMS micromachining, and double-side lithography. Its 500 ± 15 μm thickness and SEMI M1 flats ensure compatibility with precision DRIE and wafer bonding, though handling requires cleanroom protocols to preserve surface quality.
Positive
- Degenerate doping for ohmic contacts: Boron-doped to 0.001–0.005 Ω·cm (P++), providing metallic-like bulk conductivity that enables low-resistance ohmic contacts and supports cryogenic back-gated 2D FETs and electrochemical electrodes.
- Dual-side CMP for bonding and lithography: Double-side polished with Ra < 0.5 nm, facilitating double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding without additional surface preparation.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms a 1–2 nm native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench to ensure proper interface for metallization or epitaxy.
- Cleanroom handling mandatory: Wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).