| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.001–0.005 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 carrier concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.001-0.005 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (0.001–0.005 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers form a native silicon dioxide layer of approximately 1–2 nm upon ambient exposure, which must be removed prior to metallization or epitaxial processing. Unused wafers require sealed storage in a dry nitrogen cabinet or cleanroom desiccator to prevent airborne organic contamination and particulate deposition.
- Native Oxide Formation: Ambient air exposure generates a ~1–2 nm native SiO2 film that must be removed via RCA standard clean or wet processing before ohmic contact formation or epitaxy.
- Particulate and Organic Contamination Control: Storage outside a dry nitrogen cabinet or cleanroom desiccator risks airborne organic and particulate contamination that degrades the Ra < 0.5 nm polished surface.
- Edge-Only Handling Requirement: Direct contact with the polished front surface must be avoided; wafers require handling strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Wet-Chemical Processing Safety: All wet-chemical processing including RCA clean and native oxide removal must be performed inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
Preserve mirror-polished CMP surface quality and reproducible thin-film interfaces by following sequential solvent cleaning, plasma descum, and controlled storage procedures. All wet-chemical steps require exhaust fume hood or wet bench operation under institutional EHS and SDS safety protocols.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect cassette and wafer edges
Inspect the cleanroom protective cassette and wafer edges for particulate contamination or physical damage before removing any wafer. - Transfer wafer by perimeter edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and deionized water inside an exhaust fume hood or wet bench. - Dry and descum surface
Blow-dry the wafer with nitrogen gas and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform RCA standard clean or wet-chemical native oxide removal inside an exhaust fume hood or wet bench when metallization or epitaxy demands an oxide-free interface. - Store unused wafers sealed
Return unused wafers to the original cleanroom polypropylene cassette box and store sealed inside a dry nitrogen cabinet or cleanroom desiccator.
What is the carrier concentration of this 0.001–0.005 Ω·cm boron-doped silicon wafer?
The degenerately boron-doped (P++) 4-inch CZ silicon wafer with 0.001–0.005 Ω·cm resistivity corresponds to a carrier concentration of approximately 10^19–10^20 cm^-3. This heavy doping level provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and electrochemical electrodes. The resistivity range is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this SSP wafer be used for double-side alignment or backside processing?
No, this wafer is single-side polished (SSP) with a mirror-polished front (Ra < 0.5 nm) and a fine-ground back surface, so it is not suitable for double-side alignment or backside lithography. For processes requiring double-side polished surfaces, such as IR optics or fusion bonding, a DSP variant is available separately. The SSP finish is optimized for front-side thin-film deposition, photolithography, and anisotropic wet etching.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed in the original cleanroom protective cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm polished surface. Each shipment includes a lot-specific Certificate of Analysis documenting resistivity, thickness, orientation, and particle inspection (≤ 10 particles per wafer).
The 4-inch prime CZ P-type <100> silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and SSP finish (Ra < 0.5 nm) delivers a low-resistivity, crystallographically precise substrate suited for ohmic contact prototyping, cryogenic back-gated FETs, and anisotropic KOH/TMAH micromachining. Its 525 μm SEMI M1 geometry ensures compatibility with standard cassette handling and tube-furnace oxidation, though the bare surface requires immediate native-oxide management and strict cleanroom edge-handling to preserve interface quality.
Positive
- Degenerate P++ Doping for Ohmic Contacts: Boron-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), providing metallic-like bulk conductivity that supports low-resistance ohmic contacts, electrochemical electrodes, and high-power epitaxy without additional doping steps.
- SEMI M1 Geometry and CMP Finish: Standardized 100.0 ± 0.3 mm diameter, 525 ± 25 μm thickness, and Ra < 0.5 nm SSP surface ensure reproducible registration on vacuum chucks, mask aligners, and cleanroom cassettes while enabling uniform nucleation for PVD, ALD, and photoresist spin coating.
Trade-offs
- Native Oxide Requires Pre-Processing Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench under facility-approved EHS protocols before metallization or epitaxy.
- Strict Cleanroom Edge-Handling Mandate: Wafers must be handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator to prevent particulate contamination and preserve the CMP surface.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).