4-Inch N-Type Silicon Wafer 0.001-0.005 Ω·cm ATOMFAIR®

Price range: $189.00 through $409.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 100mm, 525μm, 0.001–0.005 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats, CoA included. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<110>•0.001–0.005 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <110> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing.

Sliced along the high-symmetry <110> (± 0.5°) crystal plane, the substrate exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface (at 70.5° / 109.5° in-plane angles), enabling anisotropic KOH/TMAH wet etching of atomically smooth, near-vertical (∼90°) high-aspect-ratio trench sidewalls as well as crystal-axis carrier mobility studies.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm precision orientation flat (<111> / <110> verified per lot CoA)
  • Secondary Flat: Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <110> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Length: 32.5 ± 2.5 mm•Axis: <111> / <110> flat (lot CoA verified) SEMI M1 (100 mm)
Secondary Flat Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA) SEMI M1 (100 mm <110>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Epitaxial Growth: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures clean, defect-free nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography;
  • Vertical-Sidewall MEMS & Directional Transport Devices: Perpendicular {111} etch-stop planes in <110> silicon enable vertical high-aspect-ratio KOH/TMAH microchannels, microfluidic trenches, and axis-dependent FET studies;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (110), 0.001-0.005 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type Phosphorus (0.001–0.005 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy
4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <110> Vertical-sidewall KOH MEMS & <110> lattice transport wafer
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or desiccator to avoid native oxide growth and organic contamination.

  • Cleanroom Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
  • Storage Environment: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, requiring wet processing for removal before metallization or epitaxy.
  • Surface Preservation: Preserve mirror-polished CMP cleanliness by minimizing airborne organic contamination and avoiding physical contact with the polished front surface.

Proper handling and pre-cleaning procedures are essential to maintain wafer surface quality and ensure reproducible thin-film interfaces. These steps outline the sequence for degreasing, drying, and storing wafers prior to processing.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Inspect the cleanroom protective cassette for any signs of damage or contamination before opening.
  2. Handle wafer by edge
    Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Degrease wafer surface
    Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Blow-dry the wafer with nitrogen gas to remove residual solvents and moisture.
  5. Perform plasma descum
    Perform a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Store in dry nitrogen cabinet
    Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet.

Why choose a <110> orientation N++ silicon wafer over <100> for MEMS or vertical trench fabrication?

The <110> crystal orientation exposes two sets of {111} etch-stop planes that intersect perpendicular to the wafer surface, enabling anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trench sidewalls. By contrast, <100> silicon produces sloped {111} sidewalls at 54.7°, which limits verticality in deep microfluidic channels or directional transport devices. This wafer is also degenerately phosphorus-doped to 0.001–0.005 Ω·cm (N++), providing metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates.

Can this 4-inch N-type <110> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?

Yes, the wafer is bare prime silicon with only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, LPCVD Si3N4 growth, or epitaxial deposition. However, for reproducible thin-film interfaces, the source recommends solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. Where native oxide removal or RCA standard clean is required before metallization, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols.

What are the storage and handling requirements to maintain the Ra < 0.5 nm surface of this SSP silicon wafer?

Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particulate dust. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished front surface. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit.

This 4-inch prime CZ N-type <110> silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with a CMP-polished front surface (Ra < 0.5 nm) and SEMI M1 dimensional tolerances, making it well-suited for low-resistance ohmic contact formation, anisotropic KOH/TMAH vertical-sidewall MEMS, and epitaxial prototyping. Its 525 μm thickness and bare prime surface require cleanroom-compatible handling and prompt native-oxide management before downstream processing.

Positive

  • Degenerate N++ Doping for Ohmic Contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), the substrate provides metallic-like bulk conductivity that supports low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing without additional epi doping steps.
  • <110> Orientation Enables Vertical Etch Stops: The <110> (± 0.5°) crystal plane exposes perpendicular {111} etch-stop planes, permitting anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trench sidewalls for MEMS and microfluidic structures.

Trade-offs

  • Native Oxide Requires Pre-Metallization Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench under facility-approved EHS protocols before epitaxy or metallization.
  • Cleanroom Storage and Handling Mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled strictly by the perimeter edge using vacuum wands or PTFE/PEEK tweezers to preserve the CMP surface and prevent particulate contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)