4-Inch N-Type Silicon Wafer 525μm SSP ATOMFAIR®

Price range: $169.00 through $349.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 100mm, 525±25μm, 0.1–1.0 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats. 10/25 pcs cassettes. Order now.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.1–1.0 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to 0.1–1.0 Ω·cm (~5×1015–8×1016 cm-3 electron concentration), this moderately low-resistivity n-type substrate bridges heavily doped electrode wafers and standard CMOS grades for epitaxial buffer templates, Schottky power diodes, and low-resistance MOS back gates.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.1–1.0 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>) SEMI M1 (100 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.1–1.0 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (111), 0.1-1.0 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type (0.1–1.0 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <100> Standard SEMI M1 525 μm 100 mm N-type lithography substrate
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type <100> Double-side CMP polished N-type wafer for IR optics & wafer bonding
4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <111> Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth
4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve surface quality and prevent contamination. Storage must be in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.

  • Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contact with the polished front surface.
  • Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1–2 nm in air, which must be removed before metallization or epitaxy if an oxide-free interface is required.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
  • Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Proper handling and pre-cleaning procedures are essential to preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. These steps outline the recommended sequence for degreasing, drying, and descumming prior to photoresist spin coating or PVD/ALD.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system

  1. Degrease wafer
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water.
  2. Blow-dry wafer
    Blow-dry the wafer with nitrogen gas until fully dry.
  3. Perform plasma descum
    Perform a mild oxygen plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD.
  4. Remove native oxide if required
    Remove the native oxide layer using a facility-approved wet process inside an exhaust fume hood or wet bench if an oxide-free interface is required before metallization or epitaxy.

Why choose a <111> orientation N-type silicon wafer with 0.1–1.0 Ω·cm resistivity instead of a standard <100> wafer?

The <111> orientation provides a densely packed crystal plane with hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon. Combined with the moderately low 0.1–1.0 Ω·cm phosphorus doping (~5×10^15–8×10^16 cm^-3 electron concentration), this substrate is specifically suited for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D where <100> wafers would not provide the same lattice matching or etch behavior.

Can this 4-inch N-type <111> prime silicon wafer be used directly in a tube furnace for thermal oxidation without any pre-cleaning?

Yes, the wafer is a bare prime silicon substrate with only a thin ambient native oxide (~1–2 nm) and no surface coating, allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth. However, for reproducible results, the manufacturer recommends solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. For native oxide removal or RCA standard clean before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols.

What are the storage and handling requirements to maintain the surface quality of this SSP prime silicon wafer?

Store wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the mirror-polished front surface (Ra < 0.5 nm). The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit.

This 4-inch prime CZ N-type <111> silicon wafer at 0.1–1.0 Ω·cm and 525 μm SSP offers a verified, batch-traceable substrate for hexagonal epitaxy, Schottky/ohmic prototyping, and in-house thermal oxidation, with SEMI M1 flats and sub-nanometer CMP finish supporting stepper and cassette compatibility. Its bare, single-side-polished surface and <111> orientation impose specific pre-clean, native-oxide control, and edge-handling discipline that must be matched to the intended device flow.

Positive

  • Verified <111> Hexagonal Epitaxy Platform: XRD-verified <111> ± 0.5° orientation with three-fold surface symmetry supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies. The 0.1–1.0 Ω·cm phosphorus doping provides a moderately low-resistivity n-type base for ohmic contacts and Schottky diode prototyping.
  • SEMI M1 Geometry and CMP Finish: 100.0 ± 0.3 mm diameter with SEMI M1 primary/secondary flats and Ra < 0.5 nm SSP front surface ensure reproducible registration on vacuum chucks, mask aligners, and cleanroom cassettes. TTV < 5 μm and bow/warp < 30 μm support full-wafer photolithography and PECVD/LPCVD tube processing.

Trade-offs

  • Bare Surface Requires Pre-Clean Control: The wafer is supplied bare with only a ~1–2 nm ambient native oxide; reproducible thin-film or metallization interfaces require solvent/IPA/DI cleaning, N2 dry, and optional O2 plasma descum or RCA wet clean before resist spin or PVD/ALD. All wet-chemical processing must follow institutional EHS and SDS protocols in an exhaust fume hood or wet bench.
  • Edge-Handling and Dry Storage Mandate: The mirror-polished SSP front surface and prime-grade cleanliness demand perimeter-only handling with vacuum wands or PTFE/PEEK tweezers; direct surface contact or particulate exposure compromises the Ra < 0.5 nm finish. Unused wafers must remain sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator away from dust and corrosive vapors.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.1-1.0 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)