Prime CZ N-type silicon wafer, 100mm, 300±20μm, 1–10 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•1–10 Ω·cm
Thickness:
300 ± 20 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 300 ± 20 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Doped with Phosphorus to an industry-standard 1–10 Ω·cm n-type semiconducting range (~4.5×1014–5×1015 cm-3 donor density), the wafer provides uniform majority-electron transport for PMOS/CMOS device R&D, Schottky barrier rectifiers, PECVD/ALD dielectric C-V profiling, and cleanroom thin-film deposition.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The ultra-responsive 300 ± 20 μm substrate profile enables rapid through-wafer MEMS membrane etching, thinner optical/X-ray paths, and compliant bonded device stacks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 300 ± 20 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) SEMI M1 (100 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 1-10 ohm-cm, 300 um, SSP (This Product) 4-Inch (100 mm) / SSP 300 ± 20 μm, N-Type (1–10 Ω·cm) SEMI M1 300 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <100> Standard SEMI M1 525 μm 100 mm N-type lithography substrate
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type <100> Double-side CMP polished N-type wafer for IR optics & wafer bonding
4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <111> Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth
4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom handling to preserve sub-nanometer surface quality and prevent particulate contamination. Environmental exposure to airborne organics, moisture, and corrosive vapors degrades the native oxide interface and compromises thin-film nucleation reproducibility.

  • Surface Contamination Sensitivity: The mirror-polished CMP front surface (Ra < 0.5 nm) is vulnerable to airborne molecular contamination and particulate deposition that degrade lithographic resolution and thin-film adhesion.
  • Native Oxide Formation: Bare prime silicon spontaneously forms a 1–2 nm native SiO2 layer upon air exposure, which must be removed via RCA clean or wet etching prior to epitaxial growth or ohmic metallization.
  • Mechanical Fragility: The 300 ± 20 μm substrate thickness provides limited mechanical rigidity, requiring edge-only handling with vacuum wands or PTFE/PEEK tweezers to prevent fracture and surface scratching.
  • Storage Atmosphere Requirements: Unused wafers must remain sealed in original cleanroom cassettes within a dry nitrogen cabinet or desiccator to minimize organic contamination and moisture adsorption.
  • Wet Processing Safety: All wet-chemical processing including RCA standard clean, KOH/TMAH anisotropic etching, and native oxide removal must be performed in an exhaust fume hood or wet bench under facility-approved EHS protocols.

Proper handling and pre-processing of prime-grade silicon wafers preserves surface quality and ensures reproducible device fabrication outcomes. Each step must be performed under cleanroom conditions with appropriate personal protective equipment.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or desiccator

  1. Inspect cassette packaging
    Verify the cleanroom protective cassette seal is intact and inspect wafers for visible particulate or edge damage before opening.
  2. Transfer wafer by edge
    Handle wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid contact with the polished surface.
  3. Perform solvent pre-cleaning
    Degrease wafers sequentially in acetone, electronic-grade isopropanol, and deionized water followed by nitrogen blow-drying.
  4. Apply plasma descum
    Subject wafers to mild oxygen plasma descum to remove residual organic contamination prior to photoresist spin coating or thin-film deposition.
  5. Remove native oxide if required
    Perform RCA standard clean or wet etching inside an exhaust fume hood to strip the ambient 1–2 nm native SiO2 layer before epitaxy or metallization.
  6. Store unused wafers properly
    Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet or desiccator.

What is the difference between this 300 µm 4-inch N-type wafer and the standard 525 µm version?

This wafer is specified at 300 ± 20 µm thickness, whereas the standard SEMI M1 4-inch N-type <100> wafer is 525 ± 25 µm. The thinner 300 µm profile enables faster through-wafer MEMS membrane etching, shorter optical/X-ray paths, and more compliant bonded device stacks, but it also reduces mechanical rigidity and requires more careful handling to avoid breakage. Both share the same 100.0 ± 0.3 mm diameter, N-type phosphorus doping at 1–10 Ω·cm, and <100> ± 0.5° orientation.

Can this bare prime silicon wafer be used directly for thermal oxidation or epitaxial growth without additional surface preparation?

Yes, the wafer is a bare prime silicon substrate with no deposited film or coating, carrying only a thin ambient native oxide of approximately 1–2 nm. This allows direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth. For critical interfaces such as ohmic contacts or epitaxy, the source recommends removing the native oxide via RCA standard clean or wet processing inside an exhaust fume hood or wet bench using facility-approved protocols.

What cleanroom handling and storage requirements apply to this SSP wafer with Ra < 0.5 nm surface finish?

The single-side polished front surface has a measured roughness of Ra < 0.5 nm and a particle specification of ≤ 10 particles per wafer, so it must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. Wafers ship in cleanroom protective cassettes (10 pcs or 25 pcs) that immobilize the edges; unused wafers should remain sealed in the original polypropylene cassette box inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.

The 4-inch N-type <100> prime CZ silicon wafer with 300 µm thickness and SSP finish offers a thin, low-resistivity substrate suited for MEMS membrane etching and rapid thermal processing, but its reduced thickness demands careful handling to avoid breakage and its bare surface requires in-house oxidation or cleaning before many device processes.

Positive

  • Thin 300 µm profile enables rapid etching: The 300 ± 20 µm thickness allows faster through-wafer MEMS membrane etching and shorter optical/X-ray paths compared to standard 525 µm wafers, reducing process time for bulk micromachining.
  • CMP mirror surface for uniform deposition: Single-side polished front with Ra < 0.5 nm ensures reproducible nucleation for PVD, ALD, and photoresist spin coating, supporting high-resolution lithography and thin-film growth.

Trade-offs

  • Thin substrate increases breakage risk: The 300 µm thickness makes the wafer more fragile than standard 525 µm wafers, requiring careful handling with vacuum wands or tweezers and potentially limiting use in processes with high mechanical stress.
  • Bare surface requires in-house preparation: The wafer has no pre-grown oxide or coating, so users must perform their own thermal oxidation, RCA cleaning, or native oxide removal before metallization or epitaxy, adding process steps and cleanroom infrastructure requirements.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

300 ± 20 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)