| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.001–0.005 Ω·cm |
Thickness: 300 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 300 ± 20 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The ultra-responsive 300 ± 20 μm substrate profile enables rapid through-wafer MEMS membrane etching, thinner optical/X-ray paths, and compliant bonded device stacks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 300 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) | SEMI M1 (100 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 0.001-0.005 ohm-cm, 300 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 300 ± 20 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 300 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom handling to preserve surface quality and prevent contamination. Storage must be in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy if an oxide-free interface is required.
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures are essential to preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. These steps outline the recommended sequence for preparing wafers prior to photoresist spin coating or PVD/ALD.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench
- Inspect wafer cassette
Inspect the cleanroom protective cassette for any signs of damage or particulate contamination before opening. - Handle wafer by edge
Handle the wafer strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers. - Degrease wafer surface
Degrease the wafer sequentially in acetone, electronic-grade isopropanol (IPA), and DI water. - Dry wafer with nitrogen
Dry the wafer with a nitrogen blow-dry immediately after the DI water rinse. - Perform plasma descum
Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove the native oxide via wet processing inside an exhaust fume hood or wet bench using facility-approved protocols if an oxide-free interface is required. - Store unused wafers
Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
What is the resistivity of this 4-inch N-type silicon wafer and why does it matter for ohmic contacts?
This wafer is degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++), corresponding to an electron density of approximately 10^19–10^20 cm^-3. This metallic-like bulk conductivity enables low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing without the need for additional heavy doping steps.
Can this 300 µm thick DSP wafer be used for through-wafer MEMS membrane etching and double-side lithography?
Yes. The 300 ± 20 µm thickness and dual-side mirror-polished surfaces (DSP, Ra < 0.5 nm) are specifically suited for rapid through-wafer MEMS membrane etching, double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding. The <100> crystal orientation supports KOH/TMAH anisotropic wet etching and Bosch DRIE processes.
How should these prime-grade silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the CMP mirror finish (Ra < 0.5 nm). Bare prime silicon forms a ~1–2 nm native oxide in air, so perform any native oxide removal or RCA clean immediately before metallization or epitaxy.
The 4-inch prime CZ N-type silicon wafer with degenerate phosphorus doping (0.001–0.005 Ω·cm) and dual-side CMP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts, III-V/GaN heteroepitaxy, and double-side lithography. Its 300 μm thickness and SEMI M1 flats support rapid through-wafer MEMS etching and precise cleanroom registration, though the ultra-low resistivity and bare surface demand careful handling to avoid contamination and native oxide interference.
Positive
- Degenerate doping enables ohmic contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (N++), providing metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates in high-current device testing.
- Dual-side CMP for bonding and lithography: Double-side mirror-polished surfaces (Ra < 0.5 nm) support double-sided MEMS patterning, through-wafer IR transmission, and direct fusion/anodic bonding with reproducible thin-film growth.
Trade-offs
- Native oxide requires removal before metallization: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench to ensure ohmic interface control.
- Cleanroom handling mandatory to prevent contamination: Wafers must be stored in dry nitrogen cabinets and handled by perimeter edge with vacuum wands or PTFE/PEEK tweezers to avoid particulate and organic contamination that degrades surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).