| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm |
Substrate & Dopant: CZ P-Type / Boron (B) <110>•1–10 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <110> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the high-symmetry <110> (± 0.5°) crystal plane, the substrate exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface (at 70.5° / 109.5° in-plane angles), enabling anisotropic KOH/TMAH wet etching of atomically smooth, near-vertical (∼90°) high-aspect-ratio trench sidewalls as well as enhanced in-plane hole mobility for strained PMOS and FinFET channel R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <110> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Length: 32.5 ± 2.5 mm•Axis: <111> / <110> flat (lot CoA verified) | SEMI M1 (100 mm) |
| Secondary Flat | Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA) | SEMI M1 (100 mm <110>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- Vertical-Sidewall MEMS & High Hole-Mobility Devices: Perpendicular {111} etch-stop planes in <110> silicon enable vertical high-aspect-ratio KOH/TMAH microchannels, microfluidic trenches, and high hole-mobility PMOS/FinFET studies;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (110), 1-10 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type (1–10 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve CMP surface quality and prevent particulate contamination. Storage must be in a dry nitrogen cabinet or cleanroom desiccator to avoid native oxide growth and organic contamination.
- Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Storage Atmosphere Control: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contaminants prior to deposition or lithography.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Inspect the cleanroom protective cassette for edge immobilization and absence of particulate contamination before opening. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. - Degrease sequentially
Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Blow-dry with nitrogen
Blow-dry the wafer surface with filtered nitrogen gas to remove residual solvent. - Perform plasma descum
Perform a mild O2 plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD. - Store unused wafers
Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
Why choose a <110> oriented silicon wafer over standard <100> for MEMS or FinFET research?
The <110> orientation exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface at 70.5° / 109.5° in-plane angles, enabling anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trench sidewalls. This is not achievable with <100> silicon, which etches to sloped profiles. Additionally, <110> substrates provide enhanced in-plane hole mobility, making them preferred for strained PMOS and FinFET channel R&D.
Can this 4-inch P-type <110> wafer be used for double-side lithography and wafer bonding?
Yes. The wafer features a dual-side mirror-polished (DSP) CMP finish with Ra < 0.5 nm on both surfaces, supporting double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 525 ± 25 μm thickness provides high flexural rigidity for handling during bonding processes.
What are the storage and handling requirements to maintain the CMP surface quality of this prime silicon wafer?
Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contamination. The wafers are shipped in cleanroom protective cassettes (10 pcs or 25 pcs options) designed to immobilize edges and prevent surface contact during transit.
The 4-inch P-type <110> prime CZ silicon wafer with DSP finish and 1–10 Ω·cm boron doping provides a well-characterized substrate for vertical-sidewall MEMS, high hole-mobility device studies, and double-side lithography. Its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling, though the bare surface requires strict native-oxide control and cleanroom storage to preserve the Ra < 0.5 nm finish.
Positive
- Anisotropic <110> Etch-Stop Planes: The <110> orientation exposes perpendicular {111} planes enabling KOH/TMAH etching of near-vertical high-aspect-ratio trenches and enhanced in-plane hole mobility for PMOS/FinFET R&D.
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm support double-sided lithography, IR transmission, and direct fusion or anodic wafer bonding without additional surface preparation.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS protocols before metallization or epitaxy.
- Cleanroom Storage Mandatory: To preserve the CMP finish and prevent particulate or organic contamination, wafers must remain sealed in the original cassette within a dry nitrogen cabinet or cleanroom desiccator when not in use.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).