| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•100–1000 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), P-Type (111), 100-1000 ohm-cm, 725 um, SSP (This Product) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type (100–1000 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage to prevent particulate contamination and native oxide growth. Handling must avoid surface contact, and wet processing must follow institutional EHS protocols.
- Storage Atmosphere: Store wafers sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Handling Method: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy if an oxide-free interface is required.
- Wet Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or automated wet bench following institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning steps preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. These procedures must be performed in a cleanroom environment with appropriate safety controls.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench
- Inspect packaging
Verify that the wafer cassette seal is intact and store wafers in a dry nitrogen cabinet if not immediately processed. - Handle by edge
Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge. - Pre-clean surface
Degrease wafers sequentially in electronic-grade acetone, isopropanol, and deionized water, then blow-dry with nitrogen. - Remove native oxide
Perform wet processing to remove native oxide strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store unused wafers
Keep unused wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a high-resistivity 100–1000 Ω·cm <111> silicon wafer instead of a standard 1–10 Ω·cm <100> wafer for RF or THz applications?
The 100–1000 Ω·cm Boron-doped CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, which is critical for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors. In contrast, standard 1–10 Ω·cm <100> wafers are optimized for CMOS and lithography, where lower resistivity is acceptable. Additionally, the <111> orientation provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics, benefiting GaN-on-Si epitaxy and UHV surface studies.
Can this 8-inch <111> SSP wafer be used directly in a 200 mm CMOS fabrication line?
Yes, the wafer meets SEMI M1 standards for 200 mm diameter (200.0 ± 0.2 mm), thickness (725 ± 25 μm), and V-notch fiducial along <110> ± 1°, ensuring compatibility with automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. However, the <111> orientation and high resistivity (100–1000 Ω·cm) are tailored for RF, THz, and III-nitride epitaxy rather than standard CMOS, where <100> and lower resistivity are typical. The single-side polished (SSP) finish with Ra < 0.5 nm supports uniform nucleation for epitaxy and lithography.
What are the storage and handling requirements to maintain the surface quality of this prime-grade silicon wafer?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. The wafers are supplied in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges during transit; keep unused wafers in the original cassette or FOUP carrier to minimize airborne organic contamination.
The 8-inch prime CZ P-type <111> silicon wafer with 100–1000 Ω·cm resistivity and SSP finish offers a high-resistivity, low-loss substrate for RF, THz, and GaN-on-Si epitaxy, while its SEMI M1 notch and 725 µm thickness ensure compatibility with automated 200 mm tooling. However, its <111> orientation and high resistivity require process adjustments for standard CMOS, and the bare surface demands stringent cleanroom handling to preserve the sub-nanometer polish.
Positive
- High-Resistivity Low-Loss Substrate: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors.
- <111> Orientation for Epitaxy: The <111> crystal plane provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics, supporting 200 mm GaN-on-Si/III-nitride epitaxy and UHV surface studies.
Trade-offs
- <111> Orientation Process Constraints: The <111> orientation exhibits different etch rates and surface chemistry compared to <100> silicon, requiring process optimization for standard CMOS or MEMS fabrication flows.
- Cleanroom Handling Required: Bare prime silicon with Ra < 0.5 nm surface must be handled strictly by edges using cleanroom tools and stored in dry nitrogen cabinets to prevent particle contamination and native oxide growth.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).