| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•100–1000 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), P-Type (111), 100-1000 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type (100–1000 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon substrates require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Ambient native oxide growth and particulate contamination must be controlled prior to lithography, epitaxy, or metallization.
- Atmospheric Storage Environment: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Formation: Bare prime silicon forms an ambient approximately 1–2 nm native SiO2 film in air that must be removed before metallization or epitaxy where an ohmic interface is required.
- Contact Handling Restriction: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Cassette Immobilization: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.
- Wet-Chemical Processing Containment: Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent, plasma, and oxide-control steps prior to photoresist spin coating, PVD, or ALD.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, 200 mm cleanroom polypropylene cassette or FOUP carrier, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench
- Inspect Cassette and Wafer Edges
Inspect the 200 mm cassette and wafer edges for particulate contamination or mechanical damage before removing any substrate. - Transfer by Perimeter Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge. - Degrease Sequentially
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water or apply a megasonic SC-1 clean. - Dry and Descum
Dry the surface with N2 blow-drying and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove Native Oxide Where Required
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols when an ohmic interface is required. - Return to Nitrogen Storage
Return unused wafers to the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a high-resistivity 100–1000 Ω·cm P-type <111> silicon wafer instead of standard 1–10 Ω·cm <100> for RF or THz applications?
The 100–1000 Ω·cm Boron-doped CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, which is critical for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors. In contrast, standard 1–10 Ω·cm <100> wafers have higher free-carrier absorption and dielectric loss. Additionally, the <111> orientation provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics, beneficial for GaN-on-Si epitaxy and discrete power R&D.
Can this 8-inch DSP wafer be used directly in automated 200 mm FOUP-compatible tools without additional edge trimming or cleaning?
Yes, the wafer meets SEMI M1 standards with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°). It is compatible with automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The double-side polished surface has Ra < 0.5 nm and ≤ 10 particles per wafer, ensuring cleanroom readiness.
What are the storage and handling requirements to maintain the surface quality of this prime-grade DSP silicon wafer?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges and prevent surface contact during transit.
The 8-inch prime CZ P-type <111> silicon wafer with 100–1000 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is engineered for high-frequency and optical applications where free-carrier loss and surface roughness are critical. Its SEMI M1 notch and 725 μm thickness ensure compatibility with automated 200 mm tooling, though the high-resistivity <111> orientation and bare surface demand stringent cleanroom handling and dedicated wet-processing infrastructure.
Positive
- High-Resistivity Substrate for RF and Optics: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors.
- Dual-Side CMP Finish for Bonding and Lithography: Double-side polished with Ra < 0.5 nm and TTV < 3 μm, the surface supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding with high reproducibility.
Trade-offs
- Native Oxide Requires Removal Before Critical Processes: Bare prime silicon forms a ~1–2 nm native SiO2 film in air; wet processing for native oxide removal or RCA clean must be performed in an exhaust fume hood or automated wet bench following institutional EHS protocols.
- Cleanroom Handling and Storage Mandatory: To preserve CMP cleanliness, wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.