| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Arsenic (As) <111>•0.001–0.005 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped 200 mm wafers the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Arsenic (As) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Arsenic (111), 0.001-0.005 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade arsenic-doped silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in dry nitrogen environments to minimize native oxide growth and airborne organic contamination.
- Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge or with cleanroom vacuum wands and PTFE/PEEK tweezers to avoid surface contact and particle deposition.
- Native Oxide Management: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring wet processing in exhaust fume hoods or automated wet benches when oxide removal is necessary before metallization or epitaxy.
- Storage Atmosphere Requirements: Store unused wafers sealed inside original cleanroom cassettes or FOUP carriers within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Cleanroom Compatibility: The 725 ± 25 μm thickness and SEMI M1 notch geometry are engineered for automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.
Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the surface for photoresist spin coating or PVD/ALD deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect wafer packaging integrity
Verify the cleanroom cassette seal is intact and inspect wafers for visible particulate contamination under bright-light before opening. - Transfer wafers using edge-contact tools
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact. - Perform sequential solvent degreasing
Degrease wafers sequentially in electronic-grade acetone, isopropanol, and DI water or perform megasonic/SC-1 clean. - Dry and descum the wafer surface
Blow-dry with nitrogen and apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide when required
Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store unused wafers in controlled atmosphere
Keep unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet.
Why choose arsenic-doped <111> silicon over phosphorus-doped <100> for 200 mm epitaxy and power device R&D?
Arsenic doping at 0.001–0.005 Ω·cm (N++) minimizes lattice strain and misfit dislocations because arsenic's covalent atomic radius closely matches silicon, and it diffuses roughly an order of magnitude slower than phosphorus, preserving abrupt doping profiles during high-temperature epitaxy. The <111> orientation provides hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100>, which benefits 200 mm GaN-on-Si/III-nitride epitaxy and discrete power/bipolar R&D. These combined properties make this wafer the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Can these 8-inch arsenic-doped <111> wafers be used directly in automated 200 mm FOUP and cluster tools without additional surface preparation?
Yes, the 725 ± 25 μm thickness meets SEMI M1 standards for high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°) ensures reliable optical alignment in automated handlers. However, bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so for processes requiring oxide removal or RCA clean before metallization or epitaxy, wet processing must be performed in an exhaust fume hood or automated wet bench using facility-approved protocols.
What are the storage and handling requirements to maintain the CMP surface quality of these double-side polished arsenic-doped wafers?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to preserve the Ra < 0.5 nm CMP finish and ≤ 10 particles/wafer cleanliness. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished surfaces. Keep unused wafers in the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
The 8-inch prime CZ arsenic-doped <111> silicon wafer with DSP finish and 0.001–0.005 Ω·cm resistivity provides a low-strain, low-diffusivity N++ substrate suited for 200 mm GaN-on-Si epitaxy, power device R&D, and double-side lithography. Its SEMI M1 notch geometry and 725 µm thickness ensure compatibility with automated FOUP and cluster-tool handling, though bare-surface storage and cleanroom processing protocols are mandatory to preserve the sub-nanometer CMP finish.
Positive
- Low-strain arsenic doping for epitaxy: Arsenic's covalent radius closely matches silicon, minimizing lattice strain and misfit dislocations at ultra-high doping, while its slow diffusion supports sharp doping profiles in Si/SiGe epitaxy and power MOSFET/IGBT fabrication.
- DSP finish enables double-side processing: Dual-side CMP with Ra < 0.5 nm and TTV < 3 µm supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding without additional surface preparation.
Trade-offs
- Bare surface requires cleanroom storage: Uncoated prime silicon forms a native oxide in air and is vulnerable to particulate and organic contamination; wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by edge or robotic end-effectors.
- Wet processing needs EHS infrastructure: Native oxide removal or RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or automated wet bench under facility-approved protocols, requiring institutional EHS and SDS compliance.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).