| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Arsenic (As) <100>•0.001–0.005 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped 200 mm wafers the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Arsenic (As) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Arsenic (100), 0.001-0.005 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade arsenic-doped silicon wafers require cleanroom handling to prevent particulate contamination and preserve sub-nanometer surface finish. Storage must occur in dry nitrogen or desiccator environments to minimize native oxide growth and airborne organic contamination.
- Particulate and Surface Contamination Control: Handle wafers exclusively by the perimeter edge or with cleanroom vacuum wands and PTFE/PEEK tweezers to avoid surface contact and particle deposition.
- Native Oxide Growth Management: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring controlled atmosphere storage or pre-processing native oxide removal before metallization or epitaxy.
- Cleanroom Cassette Storage Requirements: Store unused wafers sealed inside original cleanroom polypropylene cassettes or FOUP carriers within a dry nitrogen cabinet to minimize airborne organic contamination.
- Wet Processing Safety Constraints: All wet-chemical processing including RCA standard clean and native oxide removal must be performed inside an exhaust fume hood or automated wet bench following institutional EHS and SDS protocols.
Proper handling and pre-processing of prime-grade arsenic-doped silicon wafers preserves surface quality and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by native oxide control prepares wafers for lithography, epitaxy, or metallization.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator, 200 mm cleanroom polypropylene cassette or FOUP carrier
- Inspect wafer packaging integrity
Verify the cleanroom cassette seal is intact and inspect wafers for visible particulate contamination under bright-light before opening. - Transfer wafers using edge-contact tools
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact. - Perform sequential solvent degreasing
Degrease wafers sequentially in electronic-grade acetone, isopropanol, and DI water or megasonic SC-1 clean to remove organic contaminants. - Dry wafers with nitrogen blow-dry
Blow-dry cleaned wafers with filtered nitrogen gas to remove residual solvent and water without introducing particles. - Apply mild oxygen plasma descum
Apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition to ensure surface activation. - Remove native oxide before metallization
Perform wet processing for native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store unused wafers in controlled atmosphere
Seal unused wafers inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity and dopant concentration of this 8-inch arsenic-doped silicon wafer?
This wafer is N-type, Arsenic (As)-doped with a verified resistivity of 0.001–0.005 Ω·cm, corresponding to a degenerate N++ donor density of approximately 1×10^19 to 7×10^19 cm^-3. The arsenic dopant is chosen for its close covalent atomic radius match to silicon, which minimizes lattice strain and misfit dislocations at ultra-high doping, and it diffuses roughly an order of magnitude slower than phosphorus. These properties make it suitable for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Is this 200 mm arsenic-doped wafer compatible with standard FOUP cassettes and automated 200 mm cluster tools?
Yes. The wafer meets SEMI M1 specifications with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90° angle). The standard 725 μm mechanical thickness provides high flexural stiffness for automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The single-notch fiducial ensures reliable optical alignment across automated handlers and steppers.
How should I store and handle this prime-grade double-side polished arsenic-doped silicon wafer to maintain surface quality?
Store the wafer sealed inside its original cleanroom protective cassette or FOUP carrier within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished surfaces. The dual-side CMP finish (Ra < 0.5 nm) and low particle count (≤ 10 particles per wafer) are preserved by these protocols, which prevent surface contamination and mechanical damage.
The 8-inch N-type arsenic-doped prime silicon wafer delivers a degenerate 0.001–0.005 Ω·cm substrate with DSP finish (Ra < 0.5 nm) and SEMI M1 notch geometry, making it well-suited for Si/SiGe epitaxy, power device prototyping, and double-side lithography. Its low-diffusivity arsenic dopant minimizes lattice strain and autodoping during high-temperature processing, though the bare surface requires strict cleanroom handling and immediate native-oxide management before critical film deposition.
Positive
- Low-Strain Arsenic Doping for Epitaxy: Arsenic's covalent radius closely matches silicon, minimizing lattice strain and misfit dislocations at ultra-high doping levels. Its roughly order-of-magnitude slower diffusion versus phosphorus preserves abrupt doping profiles during high-temperature epitaxial and thermal processes.
- Dual-Side CMP for Bonding and Lithography: Double-side polished surfaces with Ra < 0.5 nm and TTV < 3 μm support double-sided MEMS patterning, through-wafer IR transmission, and automated fusion or anodic bonding. The SEMI M1 V-notch fiducial ensures reliable alignment in automated FOUP handlers and steppers.
Trade-offs
- Native Oxide Requires Pre-Processing Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air, which must be removed via RCA clean or wet processing before metallization or epitaxy. This step demands exhaust fume hoods or automated wet benches and strict adherence to institutional EHS protocols.
- Cleanroom Storage and Handling Mandate: Wafers must be stored sealed in dry nitrogen cabinets or cleanroom desiccators and handled only by perimeter edges with vacuum wands or PTFE/PEEK tweezers. Exposure to particulate dust or corrosive vapors compromises the CMP surface and subsequent thin-film interfaces.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).