8-Inch N-Type Silicon Wafer 100-1000 Ω·cm ATOMFAIR®

Price range: $299.00 through $1,199.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 200 mm CZ N-type silicon wafer, 725 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 V-notch. In stock.

Diameter & Notch:
8-Inch (200.0 ± 0.2 mm)
SEMI V-Notch <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•100–1000 Ω·cm
Thickness:
725 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar waveguides, IR/THz transmission windows (especially DSP), radiation/particle detector prototyping, and MEMS sensor isolation.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.

8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 8-Inch Notch & Precision

Standardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.

  • Diameter: 200.0 ± 0.2 mm (8.0 Inch)
  • Primary Fiducial: SEMI V-Notch along <110> ± 1° (Depth 1.0 +0.25/-0.00 mm, 90°)
  • Secondary Fiducial: None (SEMI M1 200 mm notch standard)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 200.0 ± 0.2 mm (8-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 725 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Fiducial (Notch) SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) SEMI M1 (200 mm)
Secondary Flat / Notch None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) SEMI M1 / Lot Laser ID
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes 200 mm Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
  • Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
  • 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
  • In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 8-Inch (200 mm), N-Type (111), 100-1000 ohm-cm, 725 um, SSP (This Product) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, P-Type <100> Standard SEMI M1 200 mm notch CMOS & lithography substrate
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) 8-Inch (200 mm) / DSP 725 ± 25 μm, P-Type <100> Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics
8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type <100> Phosphorus-doped 200 mm wafer for power & CMOS R&D
8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped 200 mm epi substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only contact to preserve CMP surface quality. Ambient native oxide growth and moisture exposure must be managed prior to downstream thermal or epitaxial processing.

  • Cleanroom Storage Atmosphere: Store wafers sealed in the original polypropylene cassette or FOUP within a dry nitrogen cabinet or cleanroom desiccator to limit airborne organic contamination and native oxide growth.
  • Particulate and Vapor Exposure: Keep substrates away from particulate dust and corrosive vapors, as surface contamination degrades the Ra < 0.5 nm polished front face and compromises thin-film nucleation uniformity.
  • Contact and Handling Restrictions: Handle strictly by the wafer perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent scratching or particle transfer to the polished surface.
  • Native Oxide Control: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxy where an oxide-free interface is required.
  • Wet-Chemical Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or automated wet bench following institutional EHS and SDS safety protocols.

Proper pre-cleaning and handling preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the substrate for photoresist coating or vacuum deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer
    Inspect the cleanroom cassette and wafer edge for particulate contamination or physical damage before removing the substrate.
  2. Transfer by Edge Contact
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease Sequentially
    Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, or perform a megasonic/SC-1 clean.
  4. Dry with Nitrogen
    Blow-dry the wafer surface with filtered nitrogen gas until no visible solvent residue remains.
  5. Apply Plasma Descum
    Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove Native Oxide if Required
    Perform RCA standard clean or wet oxide removal inside an exhaust fume hood when an oxide-free interface is required before metallization or epitaxy.
  7. Return to Nitrogen Storage
    Return unused wafers to the original cassette and store sealed within a dry nitrogen cabinet to minimize recontamination.

Why choose a high-resistivity 100–1000 Ω·cm n-type <111> silicon wafer instead of a standard 1–10 Ω·cm <100> wafer?

The 100–1000 Ω·cm phosphorus-doped n-type bulk suppresses conductive substrate coupling and parasitic RF loss, which is why this wafer is specified for RF/microwave planar waveguides, IR/THz transmission windows, radiation/particle detector prototyping, and MEMS sensor isolation. The <111> (± 0.5°) orientation adds hexagonal three-fold surface symmetry, a higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si/III-nitride epitaxy and UHV surface studies. Standard 1–10 Ω·cm <100> wafers are intended for CMOS and power R&D where low bulk resistance is acceptable.

Is this 200 mm N-type <111> prime wafer compatible with automated FOUP, stepper, and cluster-tool handling?

Yes. The wafer is manufactured to the SEMI M1 200 mm standard with a 200.0 ± 0.2 mm diameter, a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°), and the standard 725 ± 25 μm thickness, which provides the flexural stiffness required for automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The single-side-polished front surface (Ra < 0.5 nm) with TTV < 5 μm and bow/warp < 30 μm supports uniform nucleation for epitaxy, PVD/CVD, ALD, and scanner lithography. The fine-ground back surface and single-notch SEMI M1 fiducial are consistent with standard 200 mm tooling.

How should bare prime 8-inch silicon wafers be stored and handled to preserve the CMP surface before processing?

Keep unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; the supplied 200 mm cassettes (5, 10, or 25 pcs) are engineered to immobilize wafer edges and prevent surface contact during transit. Note that bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, so any wet-chemical native-oxide removal or RCA clean must be performed in an exhaust fume hood or automated wet bench following institutional EHS and SDS protocols.

The 8-inch N-type <111> prime CZ silicon wafer offers high resistivity (100–1000 Ω·cm) and a pristine CMP surface (Ra < 0.5 nm) for demanding 200 mm processes, but its <111> orientation and high resistivity impose specific constraints on epitaxial and device integration.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this wafer suppresses conductive coupling and parasitic RF loss, making it suitable for RF/microwave waveguides and radiation detector prototyping.
  • CMP Surface for Uniform Processing: The single-side polished front surface with Ra < 0.5 nm and TTV < 5 μm ensures uniform nucleation for epitaxy, lithography, and thin-film deposition across 200 mm tools.

Trade-offs

  • <111> Orientation Limits CMOS Compatibility: The <111> crystal orientation exhibits slower wet alkaline etch kinetics and different surface symmetry than <100>, which may require process adaptation for standard CMOS or MEMS fabrication.
  • Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in air, necessitating wet-chemical removal (e.g., RCA clean) before metallization or epitaxy, with strict adherence to EHS protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

5 pcs, 10 pcs, 25 pcs

Diameter

8-Inch (200.0 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

725 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)