Prime-grade 200 mm CZ N-type silicon wafer, 725 ± 25 μm, 10–20 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 V-notch. In stock.

Diameter & Notch:
8-Inch (200.0 ± 0.2 mm)
SEMI V-Notch <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•10–20 Ω·cm
Thickness:
725 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to 10–20 Ω·cm (~2×1014–4.5×1014 cm-3 electron density), this moderate-resistivity n-type substrate minimizes ionized-impurity scattering and junction capacitance, supporting MOS capacitor gate metrology, photodiode arrays, and minority-hole lifetime studies.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.

8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 8-Inch Notch & Precision

Standardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.

  • Diameter: 200.0 ± 0.2 mm (8.0 Inch)
  • Primary Fiducial: SEMI V-Notch along <110> ± 1° (Depth 1.0 +0.25/-0.00 mm, 90°)
  • Secondary Fiducial: None (SEMI M1 200 mm notch standard)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 200.0 ± 0.2 mm (8-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 725 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Fiducial (Notch) SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) SEMI M1 (200 mm)
Secondary Flat / Notch None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) SEMI M1 / Lot Laser ID
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes 200 mm Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
  • Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
  • 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (10–20 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
  • In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 8-Inch (200 mm), N-Type (111), 10-20 ohm-cm, 725 um, SSP (This Product) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type (10–20 Ω·cm) SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, P-Type <100> Standard SEMI M1 200 mm notch CMOS & lithography substrate
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) 8-Inch (200 mm) / DSP 725 ± 25 μm, P-Type <100> Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics
8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type <100> Phosphorus-doped 200 mm wafer for power & CMOS R&D
8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped 200 mm epi substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only contact to preserve CMP surface integrity. Ambient native oxide growth and environmental contaminants must be managed prior to downstream thermal or epitaxial processing.

  • Cleanroom Storage Atmosphere: Store sealed wafers in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Surface Contact Restriction: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy.
  • Wet Processing Containment: Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
  • Cassette Immobilization: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.

Chronological protocol for preserving CMP surface quality and preparing virgin silicon substrates for thin-film deposition or lithography. Steps cover inspection, pre-cleaning, native oxide control, and post-process storage.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect cassette seal and wafer edges
    Inspect the cleanroom cassette seal and wafer perimeter for particulate contamination or edge damage before opening.
  2. Transfer wafer by edge contact
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, then blow-dry with nitrogen.
  4. Apply mild oxygen plasma descum
    Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide under containment
    Remove the ambient native oxide via wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
  6. Return unused wafers to nitrogen storage
    Return unused wafers to the original cleanroom cassette or FOUP carrier and store inside a dry nitrogen cabinet.

Why choose a <111> crystal orientation n-type silicon wafer over <100> for 200 mm GaN-on-Si epitaxy?

The <111> orientation provides a densely packed three-fold surface symmetry that supports hexagonal GaN/AlN heteroepitaxy, whereas <100> silicon does not offer the same lattice matching for III-nitride growth. This wafer is oriented to <111> ± 0.5° and phosphorus-doped to 10–20 Ω·cm, which minimizes ionized-impurity scattering and junction capacitance for power/bipolar R&D. Additionally, <111> silicon exhibits slower wet alkaline etch kinetics than <100>, which can be advantageous for certain device isolation processes.

What are the total thickness variation (TTV) and bow/warp specifications for this 8-inch prime silicon wafer?

This 200 mm prime CZ silicon wafer is specified with TTV < 5 μm and bow/warp < 30 μm, as verified by non-contact optical flatness metrology. These tolerances ensure compatibility with automated 200 mm FOUP cassettes, robotic cluster tools, and lithography scanners that require tight flatness for uniform focus and overlay. The 725 ± 25 μm thickness further provides high flexural stiffness to resist sagging in horizontal wafer handling systems.

How should I store and handle this bare prime silicon wafer to prevent surface contamination?

Store the wafer sealed inside its original cleanroom protective cassette or a dry nitrogen cabinet/desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished front surface. The SSP finish with Ra < 0.5 nm is sensitive to organic contamination, so always use cleanroom-compatible gloves and tools during transfer.

This 200 mm prime CZ N-type <111> SSP wafer (10–20 Ω·cm, 725 μm) is a bare, virgin substrate engineered for 200 mm GaN-on-Si/III-nitride epitaxy, stepper lithography, and in-house oxidation or LPCVD qualification. Its value rests on SEMI M1 notch geometry, sub-nanometer CMP finish, and tight TTV/bow control, but deployment assumes cleanroom infrastructure, edge-only handling, and prompt native-oxide management before any critical interface formation.

Positive

  • SEMI M1 notch for automated 200 mm tools: Standardized 200.0 ± 0.2 mm diameter with a SEMI V-notch along <110> ± 1° (1.0 mm depth, 90°) enables reliable optical alignment across FOUP handlers, steppers, and cluster tools. The 725 ± 25 μm thickness provides the flexural stiffness expected by automated 200 mm robotic handling.
  • <111> lattice for III-nitride heteroepitaxy: The densely packed <111> (± 0.5°) plane offers three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si/AlN/SiC heteroepitaxy and discrete power/bipolar R&D. Phosphorus doping at 10–20 Ω·cm limits ionized-impurity scattering and junction capacitance for MOS capacitor and minority-carrier lifetime studies.

Trade-offs

  • Bare surface requires immediate oxide control: The SSP front side carries only a ~1–2 nm ambient native SiO2 film; any epitaxy, metallization, or ohmic contact step demands RCA/SC-1 or wet-etch removal inside an exhaust fume hood or automated wet bench under institutional EHS protocols. Delay between cleaning and deposition risks uncontrolled interfacial oxide regrowth.
  • Cleanroom storage and edge-only handling: Wafers must remain sealed in the original polypropylene cassette or FOUP within a dry nitrogen cabinet or desiccator to avoid airborne organics and particulates. Handling is restricted to perimeter edges via vacuum wands or PTFE/PEEK tweezers; surface contact or corrosive-vapor exposure compromises the Ra < 0.5 nm CMP finish.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

5 pcs, 10 pcs, 25 pcs

Diameter

8-Inch (200.0 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

725 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)