| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <111>•0.01–0.1 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+) (~1017–5×1018 cm-3 donor concentration), the wafer combines low substrate series resistance with lower free-carrier IR optical absorption than N++ substrates, supporting vertical diodes, anodic bonding, and working electrodes.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type (111), 0.01-0.1 ohm-cm, 725 um, SSP (This Product) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type (0.01–0.1 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only contact to preserve CMP surface integrity. Ambient native oxide growth and alkaline etch sensitivity dictate atmosphere and wet-processing controls.
- Cleanroom Storage Atmosphere: Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator to limit airborne organic contamination and native oxide growth.
- Edge-Only Contact Rule: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the mirror-polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring controlled wet processing before metallization or epitaxy.
- Alkaline Etch Kinetics: The <111> orientation exhibits slower wet alkaline etch kinetics than <100> silicon, which must be accounted for during anisotropic etching steps.
- Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must follow institutional EHS and SDS safety protocols inside an exhaust fume hood or automated wet bench.
Sequential cleaning and surface preparation steps preserve CMP cleanliness and reproducible thin-film interfaces. Each step must be performed under cleanroom conditions with EHS-compliant protocols.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet
- Inspect Cassette Seal
Verify the cleanroom cassette seal is intact and the wafer is free of visible particulate contamination before opening. - Transfer Wafer by Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in Solvent Sequence
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, then blow-dry with nitrogen. - Apply Plasma Descum
Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Return to Nitrogen Storage
Return unused wafers to the original cleanroom cassette and store inside a dry nitrogen cabinet to minimize recontamination.
Why choose <111> orientation over <100> for 200 mm GaN-on-Si epitaxy?
The <111> plane provides a hexagonal three-fold surface symmetry that promotes uniform nucleation for GaN/AlN heteroepitaxy, whereas <100> silicon lacks this lattice match. This wafer is oriented to <111> ± 0.5° with a dense crystal lattice, supporting 200 mm GaN-on-Si and III-nitride epitaxy. Additionally, <111> silicon exhibits slower wet alkaline etch kinetics than <100>, which can be advantageous for certain device isolation processes.
Can this 8-inch N-type <111> wafer be used for anodic bonding without additional surface preparation?
Yes, the wafer is supplied as bare prime silicon with a single-side polished (SSP) front surface (Ra < 0.5 nm) and fine-ground back, making it suitable for anodic bonding as-is. The low resistivity of 0.01–0.1 Ω·cm (N+) ensures low substrate series resistance, which facilitates uniform current distribution during bonding. However, for optimal bond quality, standard cleanroom cleaning to remove ambient native oxide (~1–2 nm) is recommended.
What are the storage and handling requirements to maintain the surface quality of this prime silicon wafer?
Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator to prevent particle contamination and native oxide growth beyond the ambient 1–2 nm. Handle only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished surface. The cassettes are designed to immobilize wafer edges and prevent surface contact during transit and storage.
The 8-inch prime CZ N-type <111> silicon wafer (0.01–0.1 Ω·cm, 725 μm SSP) delivers a low-resistivity, densely packed <111> substrate suited to 200 mm GaN/III-nitride epitaxy, vertical diodes, and anodic bonding, with SEMI M1 notch geometry and sub-nanometer CMP finish for automated FOUP and scanner compatibility. Its bare, uncoated surface and <111> orientation impose specific pre-clean, native-oxide control, and etch-rate considerations that must be engineered into downstream process flows.
Positive
- Low-resistivity N+ substrate: Phosphorus doping at 0.01–0.1 Ω·cm (~10^17–5×10^18 cm^-3) lowers substrate series resistance while exhibiting less free-carrier IR absorption than N++ material, benefiting vertical diodes, anodic bonding, and working-electrode designs.
- <111> lattice for III-nitride epitaxy: The <111> (± 0.5°) orientation provides hexagonal three-fold surface symmetry and higher in-plane elastic modulus along key cleavage directions, supporting 200 mm GaN-on-Si/AlN/SiC heteroepitaxy and UHV surface studies.
- SEMI M1 200 mm tool compatibility: Standardized 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and SEMI V-notch along <110> ± 1° enable reliable alignment across FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.
- CMP mirror finish for thin films: Single-side polished front with Ra < 0.5 nm, TTV < 5 μm, and bow/warp < 30 μm supports uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography.
Trade-offs
- Native oxide requires pre-clean control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; native oxide removal or RCA standard clean before metallization or epitaxy must be performed in an exhaust fume hood or automated wet bench under facility-approved protocols.
- <111> slower alkaline etch kinetics: The densely packed <111> plane exhibits slower wet alkaline etch kinetics than <100> silicon, which must be accounted for when designing anisotropic etch processes or release steps.
- Cleanroom storage and handling required: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handled strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.