| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•100–1000 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar waveguides, IR/THz transmission windows (especially DSP), radiation/particle detector prototyping, and MEMS sensor isolation.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type (100), 100-1000 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (100–1000 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulate contamination, corrosive vapors, and uncontrolled humidity must be minimized during storage and processing.
- Cleanroom Storage Requirements: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Protocol: Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient approximately 1–2 nm native SiO2 film in air that must be removed before metallization or epitaxy.
- Wet Processing Containment: Perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
- Cassette Immobilization: Keep unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, native oxide control, and proper cassette storage to maintain wafer quality.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet, FOUP carrier
- Inspect wafer cassette
Verify the cleanroom protective cassette is sealed and free of particulate contamination before opening. - Handle by perimeter edge
Transfer wafers using cleanroom vacuum wands or PTFE/PEEK tweezers while handling strictly by the perimeter edge. - Degrease sequentially
Degrease wafers sequentially in electronic-grade acetone, isopropanol, and DI water or perform megasonic/SC-1 clean. - Dry and descum
Blow-dry with N2 and apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store unused wafers
Keep unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet.
What is the resistivity range of this 8-inch N-type silicon wafer and how does it affect RF device performance?
This wafer is Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm, as measured by four-point probe. This high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar waveguides and IR/THz transmission windows. The wide resistivity range provides flexibility for detector prototyping and MEMS sensor isolation.
Is this 200 mm silicon wafer compatible with automated FOUP cassettes and cluster tools?
Yes, the wafer meets SEMI M1 standards with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°). These specifications ensure reliable optical alignment and handling across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The high flexural stiffness of the 725 μm thickness supports mechanical stability during automated processing.
How should I store and handle these prime-grade silicon wafers to maintain surface cleanliness?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges and prevent surface contact during transit.
The 8-inch prime CZ N-type <100> silicon wafer with 100–1000 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is engineered for high-resistivity RF, detector, and MEMS applications where conductive substrate coupling must be suppressed. Its SEMI M1 200 mm geometry and 725 μm thickness ensure compatibility with automated FOUP-based tooling, though the high resistivity and bare surface demand careful cleanroom handling to preserve interface quality.
Positive
- High-Resistivity N-Type Substrate: Phosphorus doping at 100–1000 Ω·cm suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar waveguides, IR/THz transmission windows, and radiation detector prototyping.
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm and TTV < 3 μm enable reproducible thin-film growth, double-sided lithography, and automated fusion/anodic bonding for MEMS and advanced packaging.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air; wet-chemical removal (e.g., RCA clean) must be performed in an exhaust fume hood or automated wet bench following institutional EHS protocols before metallization or epitaxy.
- Cleanroom Storage and Handling: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by perimeter edges with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).