Prime CZ P-Type silicon wafer, 150.0 ± 0.3 mm, 675 ± 25 μm, 1–10 Ω·cm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•1–10 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 150 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat None (SEMI M1 standard for 150 mm P-type <111>) SEMI M1 (150 mm P<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), P-Type (111), 1-10 ohm-cm, 675 um, DSP (This Product) 6-Inch (150 mm) / DSP 675 ± 25 μm, P-Type (1–10 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <100> Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, P-Type <100> Double-side CMP polished 150 mm wafer for bonding & IR optics
6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <111> Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D
6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & <110> hole-mobility wafer

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and handling to preserve CMP surface quality and prevent particulate contamination. Environmental exposure to airborne organics, moisture, and corrosive vapors must be minimized to avoid degradation of the native oxide and surface finish.

  • Cleanroom Storage Requirements: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling Protocol: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and contamination.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for native oxide removal before metallization or epitaxy.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.

Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to photoresist coating or deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect cassette packaging
    Verify the cleanroom protective cassette is sealed and undamaged before opening in a controlled environment.
  2. Handle by perimeter edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge.
  3. Degrease in solvent sequence
    Immerse wafers sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic contaminants.
  4. Dry with nitrogen
    Blow-dry the wafer surface with filtered N2 gas until no visible solvent residue remains.
  5. Perform plasma descum
    Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Store unused wafers
    Return unused wafers to the original cleanroom cassette and store within a dry nitrogen cabinet to minimize airborne contamination.

Why choose a <111> oriented silicon wafer over <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched GaN, AlN, and SiC heteroepitaxy, whereas <100> is preferred for standard CMOS. This wafer is Boron-doped to 1–10 Ω·cm with a <111> (± 0.5°) orientation verified by XRD, and its higher in-plane elastic modulus and slower wet alkaline etch kinetics make it suitable for discrete power/bipolar R&D and UHV surface reconstruction studies. However, <111> silicon exhibits different cleavage behavior and is not the standard choice for high-mobility MOSFET channels.

Can this double-side polished (DSP) 6-inch wafer be used for direct wafer bonding and through-wafer IR transmission?

Yes, the dual-side mirror-polished surfaces with Ra < 0.5 nm (CMP finish) are specifically designed for direct fusion and anodic bonding, as well as double-sided MEMS patterning and through-wafer infrared transmission. The 675 ± 25 μm thickness and TTV < 3 μm ensure flatness compatible with bonding interfaces. For optimal results, store wafers in a dry nitrogen cabinet and handle only by the edge to preserve surface cleanliness.

What are the storage and handling requirements to maintain the prime-grade surface of this 150 mm silicon wafer?

Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent native oxide growth and organic contamination. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; the supplied cleanroom protective cassettes (10 pcs or 25 pcs) immobilize edges during transit. Prior to processing, a solvent clean (acetone, IPA, DI water) followed by N2 dry and mild O2 plasma descum is recommended to preserve the Ra < 0.5 nm surface.

This 6-inch prime CZ P-type <111> silicon wafer combines a dual-side CMP finish (Ra < 0.5 nm) with SEMI M1 675 μm geometry and 1–10 Ω·cm boron doping, making it well-suited for double-side lithography, fusion bonding, and hexagonal GaN/AlN/SiC heteroepitaxy. Its bare, uncoated surface and <111> orientation, however, impose strict cleanroom handling and wet-bench protocols to preserve the native-oxide interface and mirror finish.

Positive

  • Dual-Side CMP Mirror Finish: DSP surfaces with Ra < 0.5 nm enable double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding without additional polishing.
  • <111> Lattice for Hexagonal Epitaxy: The densely packed three-fold <111> plane supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar R&D.

Trade-offs

  • Bare Surface Requires Cleanroom Handling: Uncoated prime silicon forms a ~1–2 nm native oxide in air and must be stored in dry nitrogen cabinets and handled only by edge with vacuum wands or PTFE/PEEK tweezers.
  • Wet Processing Needs EHS Infrastructure: Native-oxide removal or RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)