Prime CZ P-Type/Boron 6-inch silicon wafer, 0.001–0.005 Ω·cm, 675 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•0.001–0.005 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 hole concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 150 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat None (SEMI M1 standard for 150 mm P-type <111>) SEMI M1 (150 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), P-Type (111), 0.001-0.005 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type (0.001–0.005 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <100> Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, P-Type <100> Double-side CMP polished 150 mm wafer for bonding & IR optics
6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <111> Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D
6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & <110> hole-mobility wafer

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only contact to preserve the CMP mirror finish. Ambient native oxide growth and airborne organic contamination must be managed prior to lithography, epitaxy, or metallization.

  • Atmospheric Storage Environment: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Formation: Bare prime silicon develops an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
  • Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols inside an exhaust fume hood or wet bench.
  • Organic Contamination Control: Minimize airborne organic contamination by keeping unused wafers sealed in the original cassette box when not actively processed.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain wafer surface integrity.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before removing any wafer.
  2. Transfer Wafer by Perimeter Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and Plasma Descum
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove Native Oxide if Required
    Perform RCA standard clean or wet oxide removal inside an exhaust fume hood or wet bench when native oxide removal is required before metallization or epitaxy.
  6. Store Unused Wafers Sealed
    Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet.

Why choose a <111> orientation P++ silicon wafer over standard <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed three-fold symmetric surface that supports lattice-matched III-nitride heteroepitaxy (GaN, AlN, SiC) and exhibits slower wet alkaline etch kinetics than <100> silicon. Combined with degenerate boron doping at 0.001–0.005 Ω·cm (P++), it enables low-resistance ohmic contacts and metallic-like bulk conductivity for cryogenic back-gated 2D FETs and high-power epitaxy. Standard <100> wafers are preferred for CMOS lithography, whereas this <111> P++ substrate is optimized for hexagonal epitaxy and discrete power/bipolar R&D.

Can this 6-inch P++ <111> wafer be used directly in a 150 mm photolithography stepper without additional surface preparation?

Yes, the wafer is SEMI M1 compliant with a 150.0 ± 0.3 mm diameter, 675 ± 25 μm thickness, and a primary flat of 57.5 ± 2.5 mm along <110> ± 1°, ensuring compatibility with automated 150 mm steppers, PECVD/LPCVD cassettes, and robotic handling chucks. The single-side polished front surface has Ra < 0.5 nm and carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial growth. For optimal lithography, standard solvent pre-cleaning (acetone, IPA, DI water) and O2 plasma descum are recommended to remove organic contaminants.

What are the storage and handling requirements to maintain the surface quality of these prime-grade silicon wafers?

Wafers must be stored sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator to prevent particulate contamination and native oxide growth beyond the ambient ~1–2 nm. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. Each shipment includes a Certificate of Analysis (CoA) documenting resistivity, thickness, orientation, and particle inspection (≤ 10 particles per wafer), ensuring traceability for institutional cleanroom protocols.

The 6-inch P-type <111> prime CZ silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and SSP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts and hexagonal heteroepitaxy, but its <111> orientation and high doping level impose specific constraints on etch processing and native oxide management.

Positive

  • Degenerate doping enables ohmic contacts: Boron-doped to 0.001–0.005 Ω·cm (P++), providing metallic-like bulk conductivity suitable for low-resistance ohmic contacts and cryogenic back-gated 2D FETs.
  • <111> lattice supports hexagonal epitaxy: The densely packed <111> crystal plane exhibits three-fold surface symmetry and slower wet alkaline etch kinetics than <100>, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies.

Trade-offs

  • <111> orientation limits CMOS compatibility: The <111> crystal orientation is not standard for CMOS lithography, which typically uses <100> wafers; this restricts direct use in mainstream CMOS pilot lines without process adaptation.
  • Native oxide requires removal before metallization: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet processing for native oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)