6-Inch N-Type Silicon Wafer 0.001-0.005 Ω·cm SSP ATOMFAIR®

Price range: $339.00 through $749.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 150.0 ± 0.3 mm, 675 ± 25 μm, 0.001–0.005 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•0.001–0.005 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>) SEMI M1 (150 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type (100), 0.001-0.005 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type (0.001–0.005 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <100> Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, P-Type <100> Double-side CMP polished 150 mm wafer for bonding & IR optics
6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <111> Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D
6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & <110> hole-mobility wafer

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage in a dry nitrogen cabinet or desiccator is necessary to minimize native oxide growth and maintain surface quality.

  • Cleanroom Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
  • Storage Environment: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, which may require removal before metallization or epitaxy.
  • Wet Processing Safety: Perform wet-chemical processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety guidelines.

Proper handling and pre-cleaning steps are essential to preserve the mirror-polished surface and ensure reproducible thin-film interfaces. These procedures should be performed in a cleanroom environment following institutional safety protocols.

Required Equipment: Cleanroom vacuum wands, PTFE/PEEK tweezers, Exhaust fume hood or wet bench

  1. Inspect wafer
    Inspect the wafer for visible particles or damage under bright light before handling.
  2. Handle by edge
    Handle the wafer strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Pre-clean wafer
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol (IPA), and DI water.
  4. Dry wafer
    Blow-dry the wafer with nitrogen gas to remove residual solvents.
  5. Descum surface
    Perform a mild O2 plasma descum to remove organic contaminants prior to photoresist spin coating or PVD/ALD.
  6. Store wafer
    Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

What is the resistivity of this 6-inch N-type silicon wafer and why does it matter for ohmic contacts?

This wafer is degenerately Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm (N++), corresponding to an electron density of approximately 10^19–10^20 cm^-3. This metallic-like bulk conductivity is specifically engineered for low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing. The resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.

Can this 150 mm N-type <100> wafer be used for KOH anisotropic etching and CMOS pilot-line processing?

Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, as well as Bosch DRIE and epitaxial layer growth. The SEMI M1 675 ± 25 μm thickness provides high flexural stiffness for automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, and robotic handling chucks, making it suitable for MEMS, CMOS, and power device prototyping.

How should these bare prime silicon wafers be stored and handled to preserve the CMP surface?

Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm mirror-polished front surface. Bare prime silicon forms a ~1–2 nm native oxide in air; perform any native oxide removal or RCA clean inside an exhaust fume hood or wet bench following institutional EHS protocols.

This 6-inch prime CZ N-type <100> silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with a sub-nanometer CMP front surface and SEMI M1 675 μm geometry, making it well-suited for low-resistance ohmic contact formation, III-V/GaN heteroepitaxy, and 150 mm pilot-line lithography. Its bare, uncoated surface and SSP-only finish, however, require the buyer to manage native oxide growth and backside handling within a cleanroom infrastructure.

Positive

  • Degenerate N++ Doping for Ohmic Contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), the substrate provides metallic-like bulk conductivity that supports low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing without additional epitaxial doping steps.
  • CMP Mirror Surface for Thin-Film Growth: The single-side polished front surface with Ra < 0.5 nm and ≤10 particles per wafer ensures uniform nucleation for ALD, PVD, and epitaxial growth, while the SEMI M1 675 ± 25 μm thickness maintains flexural stiffness across automated 150 mm steppers and cassette handling.

Trade-offs

  • Native Oxide Requires Pre-Metallization Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; reproducible ohmic interfaces or epitaxial growth demand RCA cleaning or wet oxide removal in an exhaust fume hood or wet bench prior to deposition.
  • SSP Backside Limits Bonding Applications: The fine-ground back surface is not CMP-polished, so the wafer is unsuitable for direct wafer bonding, through-silicon via reveal, or backside lithography that requires a mirror finish on both faces.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)