| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.01–0.1 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 76.2 mm P<100>) | SEMI M1 (76.2 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (100), 0.01-0.1 ohm-cm, 380 um, SSP (This Product) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type (0.01–0.1 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate contamination, airborne organics, and corrosive vapors. Storage and handling must preserve the CMP mirror finish and prevent surface contact.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
- Particulate and Organic Contamination Control: Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination.
- Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and contamination.
- Corrosive Vapor Exposure: Keep wafers away from particulate dust and corrosive vapors that can degrade the polished surface and alter surface chemistry.
- Wet Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the surface for photoresist spin coating or PVD/ALD.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect Cassette Seal
Verify the 25-wafer polypropylene cassette remains sealed and stored in a dry nitrogen cabinet before opening. - Handle by Perimeter Edge
Transfer wafers individually using a cleanroom vacuum wand or PTFE/PEEK tweezers contacting only the perimeter edge. - Degrease Sequentially
Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood. - Dry with Nitrogen
Blow-dry the wafer surface with filtered N2 to remove residual solvent and water. - Perform Plasma Descum
Apply a mild O2 plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide if Required
Perform RCA standard clean or wet oxide removal inside an exhaust fume hood using facility-approved protocols when metallization or epitaxy demands an oxide-free interface. - Return Unused Wafers to Storage
Seal unused wafers inside the original polypropylene cassette box within a dry nitrogen cabinet to prevent recontamination.
What is the resistivity range of this 3-inch P-type boron-doped silicon wafer?
This wafer is Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm (P+), measured by four-point probe (4PP). This low-resistivity range provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.
Can this 3-inch SSP wafer be used for KOH anisotropic wet etching and DRIE MEMS micromachining?
Yes. The wafer is sliced along the <100> (± 0.5°) crystal plane, which supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE). The cubic <100> surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, making it suitable for MEMS and anisotropic silicon micromachining.
How should these bare prime silicon wafers be stored and handled to preserve the CMP surface?
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers sealed in the original polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
The 3-inch P-type <100> prime CZ silicon wafer with 0.01–0.1 Ω·cm boron doping and SSP finish (Ra < 0.5 nm) offers a low-resistivity, crystallographically precise substrate suited for MEMS anisotropic etching, thin-film deposition, and electrochemical electrode prototyping. Its 380 μm thickness and SEMI M1 flats ensure compatibility with standard 3-inch cleanroom tools, though handling requires strict cleanroom protocols and the bare surface demands controlled native-oxide management.
Positive
- Low-Resistivity P+ Substrate: Boron doping at 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction and ohmic contact formation, while reducing free-carrier infrared absorption compared to degenerately doped P++ alternatives.
- CMP Mirror Surface for Lithography: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, and high-resolution photoresist spin coating, supporting reproducible thin-film growth and sub-micron patterning.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols before metallization or epitaxy.
- Cleanroom Handling Mandatory: To preserve CMP cleanliness, wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers; particulate or organic contamination will degrade surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).