| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•1–10 Ω·cm |
Thickness: 500 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 500 ± 20 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The thinned 500 ± 20 μm profile accelerates through-wafer DRIE/wet etching across 150 mm substrates, improves thermal transfer during rapid thermal processing (RTP), and increases mid/far-infrared optical transmission. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 500 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) | SEMI M1 (150 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 1-10 ohm-cm, 500 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 500 ± 20 μm, P-Type (1–10 Ω·cm) | SEMI M1 500 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only contact to preserve CMP surface integrity. Ambient native oxide growth and environmental contaminants must be managed prior to critical thin-film or lithographic processing.
- Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination and particulate deposition.
- Edge-Only Contact Protocol: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface scratching and particle transfer to the polished face.
- Native Oxide Awareness: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxial growth.
- Wet-Chemical Processing Environment: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS/SDS safety guidelines.
Proper handling and pre-cleaning of prime CZ silicon wafers preserves CMP surface quality and ensures reproducible thin-film interfaces. Sequential solvent cleaning, plasma descum, and controlled storage prevent contamination during device fabrication.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect wafer cassette
Inspect the cleanroom cassette for particulate contamination and verify that wafers are immobilized without edge contact before opening. - Transfer wafer by edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water followed by N2 blow-drying. - Apply mild O2 plasma descum
Apply a mild O2 plasma descum to the wafer surface prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove the ambient native SiO2 film via RCA standard clean or wet processing inside an exhaust fume hood when preparing for metallization or epitaxy. - Store unused wafers sealed
Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the difference between this 500 µm DSP wafer and the standard 675 µm SSP 6-inch P-type <100> wafer?
This wafer is a 500 ± 20 µm double-side polished (DSP) substrate, whereas the standard 6-inch P-type <100> wafer is 675 ± 25 µm and single-side polished (SSP). The thinner 500 µm profile accelerates through-wafer DRIE and wet etching, improves thermal transfer during rapid thermal processing, and increases mid/far-infrared optical transmission. The DSP finish (Ra < 0.5 nm on both sides) additionally supports double-sided lithography, through-wafer IR transmission, and direct fusion or anodic bonding, which are not possible with an SSP backside.
Can this 6-inch P-type <100> prime silicon wafer be used for KOH anisotropic etching and CMOS pilot-line prototyping?
Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, as well as Bosch DRIE and epitaxial layer growth. The Boron-doped 1–10 Ω·cm resistivity provides a well-characterized majority-hole carrier profile suitable for MOSFET/CMOS device prototyping, Schottky barrier testing, and C-V metrology. The wafer is prime-grade and virgin, with a thin ambient native oxide (~1–2 nm) that allows direct in-house thermal oxidation or epitaxial growth.
How should these 6-inch prime silicon wafers be stored and handled to maintain surface quality before cleanroom processing?
Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the mirror-polished CMP surfaces (Ra < 0.5 nm). Prior to photoresist spin coating or PVD/ALD, degrease sequentially in acetone, electronic-grade IPA, and DI water, followed by N2 blow-drying and a mild O2 plasma descum.
The 6-inch prime CZ P-type <100> silicon wafer with DSP finish and 500 µm thickness offers a well-characterized substrate for CMOS prototyping, MEMS, and thin-film metrology, but its thin profile demands careful handling and cleanroom storage to avoid breakage and contamination.
Positive
- Dual-side CMP finish: Double-side polished surfaces with Ra < 0.5 nm enable reproducible thin-film growth, lithography, and direct wafer bonding.
- Thin 500 µm profile: The 500 ± 20 µm thickness accelerates through-wafer etching and improves thermal transfer during RTP, while enhancing mid/far-IR transmission.
Trade-offs
- Fragile thin substrate: At 500 µm thickness, wafers are more prone to breakage during handling and processing compared to standard 675 µm wafers, requiring careful edge handling with vacuum wands or tweezers.
- Native oxide and contamination control: Bare silicon forms a native oxide (~1–2 nm) and is sensitive to particulate and organic contamination; storage in dry nitrogen cabinets and cleanroom protocols are mandatory to preserve surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).