| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.001–0.005 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 hole concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) | SEMI M1 (150 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 0.001-0.005 ohm-cm, 675 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type (0.001–0.005 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom-compatible storage and handling to preserve surface quality. Environmental exposure to particulates, corrosive vapors, and moisture must be minimized to prevent contamination and native oxide growth.
- Cleanroom Storage Requirements: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Protocol: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for oxide removal before metallization or epitaxy.
- Wet Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety guidelines.
Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to photoresist coating or deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer cassette
Verify that the cleanroom protective cassette is sealed and free from visible particulate contamination before opening. - Handle by perimeter edge
Transfer wafers individually using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge. - Degrease sequentially
Immerse wafers sequentially in acetone, electronic-grade isopropanol, and deionized water to remove organic residues. - Dry with nitrogen
Blow-dry the wafer surface with filtered nitrogen gas until all visible liquid is removed. - Perform plasma descum
Apply a mild O2 plasma descum to the wafer surface prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet.
What is the resistivity of this 6-inch P-type boron-doped silicon wafer and what does it mean for ohmic contacts?
This wafer is degenerately Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm (P++), corresponding to a hole concentration of approximately 10^19–10^20 cm^-3. This metallic-like bulk conductivity is specifically suited for forming low-resistance ohmic contacts, as well as for cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy. The resistivity is measured by four-point probe (4PP) and documented on the batch Certificate of Analysis.
Can this 6-inch DSP silicon wafer be used for double-side lithography and wafer bonding?
Yes. The wafer features a dual-side mirror-polished (DSP) finish with a CMP surface roughness of Ra < 0.5 nm, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The SEMI M1 standard 675 ± 25 μm thickness provides the mechanical rigidity required for automated 150 mm photolithography steppers and bonding equipment.
How should these prime-grade silicon wafers be stored and handled to maintain surface cleanliness?
Wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs) that immobilize the wafer edges and prevent surface contact. Store sealed cassettes inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the Ra < 0.5 nm CMP finish and the ≤ 10 particles per wafer cleanliness specification.
The 6-inch prime CZ P-type <100> silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and dual-side CMP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, and double-side lithography. Its SEMI M1-compliant 675 μm thickness ensures compatibility with automated 150 mm tooling, though the bare surface requires strict cleanroom handling and immediate native-oxide management before critical downstream processing.
Positive
- Degenerate P++ Doping for Ohmic Contacts: Boron-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), providing metallic-like bulk conductivity that enables low-resistance ohmic contacts and supports cryogenic back-gated 2D FET and electrochemical electrode applications.
- Dual-Side CMP Mirror Finish: Double-side polished with Ra < 0.5 nm, facilitating double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding without additional surface preparation.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet-chemical removal (e.g., RCA clean) must be performed in an exhaust fume hood or wet bench under institutional EHS protocols before metallization or epitaxy.
- Cleanroom Handling Mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and preserve surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).