| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•1–10 Ω·cm |
Thickness: 625 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 625 ± 20 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The 625 ± 20 μm precision-tolerance thickness suits 150 mm MEMS micromachining, double-side alignment lithography, Bosch DRIE through-etching, and wafer bonding with tight cavity depth control. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 625 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) | SEMI M1 (150 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 1-10 ohm-cm, 625 um, SSP (This Product) | 6-Inch (150 mm) / SSP | 625 ± 20 μm, P-Type (1–10 Ω·cm) | SEMI M1 625 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage to prevent particulate contamination and native oxide growth. Handling must avoid surface contact to preserve the sub-nanometer CMP finish and prevent fracture of the 625 μm substrate.
- Storage Atmosphere: Store wafers sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Surface Contact Prevention: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing inside an exhaust fume hood or wet bench for removal before metallization or epitaxy.
- Mechanical Fragility: The 625 ± 20 μm thickness and 150 mm diameter make the wafer susceptible to fracture if subjected to uneven mechanical stress during cassette loading or vacuum chucking.
Proper handling preserves the CMP surface finish and prevents contamination during device fabrication. Sequential cleaning and controlled environment processing ensure reproducible thin-film interfaces.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect Cassette Seal
Verify the cleanroom protective cassette is sealed and undamaged before opening in a controlled environment. - Transfer Wafer
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge. - Pre-Clean Surface
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water, followed by N2 blow-drying and mild O2 plasma descum. - Remove Native Oxide
Perform wet processing for native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols. - Store Unused Wafers
Return unused wafers to the original cleanroom polypropylene cassette box and store in a dry nitrogen cabinet to minimize airborne organic contamination.
What is the difference between this 625 µm 6-inch silicon wafer and the standard 675 µm version?
This wafer is specified at 625 ± 20 µm thickness, whereas the standard SEMI M1 6-inch wafer is 675 ± 25 µm. The thinner 625 µm substrate is intended for applications requiring tighter cavity depth control, such as MEMS micromachining, double-side alignment lithography, and wafer bonding, where the reduced thickness aids in through-etching and depth uniformity. Both wafers share the same 150.0 mm diameter, P-type boron doping (1–10 Ω·cm), and <100> orientation, but the thickness tolerance and nominal value differ to suit specific process requirements.
Can this SSP wafer be used for double-side processing or wafer bonding without additional surface preparation?
This wafer is single-side polished (SSP) with a mirror-polished front surface (Ra < 0.5 nm) and a fine-ground back surface. For double-side alignment lithography or wafer bonding, the back surface may require additional polishing or cleaning to achieve the necessary flatness and surface quality. The front surface is ready for thin-film deposition, photolithography, and thermal oxidation, but processes requiring both sides to be polished should consider a double-side polished (DSP) wafer instead.
What are the storage and handling requirements to maintain the surface quality of this prime silicon wafer?
Store wafers sealed in their original cleanroom protective cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the polished surface. The wafers are shipped in cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.
The 6-inch prime CZ P-type <100> silicon wafer with 625 μm thickness and SSP finish offers a well-characterized substrate for MEMS, CMOS prototyping, and thin-film metrology, though its single-side polish and bare silicon surface impose specific handling and cleaning requirements.
Positive
- Precision thickness for MEMS and bonding: The 625 ± 20 μm thickness tolerance supports double-side alignment lithography, Bosch DRIE through-etching, and wafer bonding with tight cavity depth control.
- CMP mirror surface for uniform deposition: Single-side polished front with Ra < 0.5 nm ensures reproducible nucleation for epitaxy, PVD, ALD, and high-resolution 150 mm stepper lithography.
Trade-offs
- Single-side polish limits backside processes: The fine-ground back surface may not be suitable for processes requiring double-side polished (DSP) substrates, such as backside alignment or IR optics.
- Native oxide requires removal before critical steps: Bare prime silicon forms a ~1–2 nm native SiO2 film in air, necessitating wet processing (e.g., RCA clean) in a fume hood prior to metallization or epitaxy.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).