| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.1–1.0 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 0.1–1.0 Ω·cm (~2×1016–2×1017 cm-3 acceptor concentration), this moderately low-resistivity substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.1–1.0 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) | SEMI M1 (150 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (0.1–1.0 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 0.1-1.0 ohm-cm, 675 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type (0.1–1.0 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers require cleanroom handling to prevent particulate contamination and preserve sub-nanometer surface roughness. Ambient exposure forms a native silicon dioxide layer that must be removed before epitaxy or metallization.
- Particulate and Organic Contamination Control: Store unused wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic and particulate contamination.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native silicon dioxide film in air, requiring wet-chemical removal before epitaxial growth or ohmic contact formation.
- Edge-Contact Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the dual-side mirror-polished surfaces.
- Corrosive Vapor and Dust Exposure: Store wafers away from particulate dust and corrosive vapors that can degrade the CMP surface finish and alter surface chemistry.
Proper handling preserves the dual-side CMP finish and prevents contamination that degrades thin-film growth and lithography reproducibility. Surface preparation removes organic residues and native oxide before critical process steps.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect cassette packaging
Verify the cleanroom protective cassette is sealed and undamaged before opening in a controlled environment. - Transfer wafer by edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water. - Dry with nitrogen
Dry the wafer with a nitrogen blow-dry to remove residual solvent and water. - Descum with oxygen plasma
Apply a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide in wet bench
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols. - Store unused wafers sealed
Return unused wafers to the original cleanroom cassette and store within a dry nitrogen cabinet.
What is the resistivity range and dopant type of this 6-inch silicon wafer?
This wafer is P-Type, Boron-doped with a resistivity of 0.1–1.0 Ω·cm, corresponding to an acceptor concentration of approximately 2×10^16–2×10^17 cm^-3. The resistivity is verified by four-point probe (4PP) per batch and documented on the Certificate of Analysis. This moderately low-resistivity range bridges heavily doped electrode wafers and standard CMOS grades.
Is this wafer compatible with double-side lithography and wafer bonding processes?
Yes. The wafer features a double-side polished (DSP) CMP finish with Ra < 0.5 nm on both surfaces, enabling double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The <100> crystal orientation and 675 ± 25 μm thickness provide the mechanical stability required for these processes.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed in the original cleanroom protective cassette inside a dry nitrogen cabinet or desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination. The wafers are supplied in 10 pcs or 25 pcs cassettes designed to immobilize edges during transit.
The 6-inch prime CZ P-type boron-doped silicon wafer (0.1–1.0 Ω·cm, <100>, 675 μm, DSP) offers a dual-side mirror-polished, low-resistivity substrate suited for epitaxial templates, power device prototyping, and double-side lithography; however, its moderately low resistivity range and bare silicon surface require careful cleanroom handling and wet-chemical processing to preserve interface quality.
Positive
- Dual-side CMP mirror finish: Double-side polished surfaces with Ra < 0.5 nm enable reproducible thin-film growth, double-sided MEMS patterning, and direct fusion or anodic bonding.
- Low-resistivity epitaxial template: Boron doping at 0.1–1.0 Ω·cm provides a moderately low-resistivity base for epitaxial growth, ohmic contacts, and low-resistance MOS back gates.
Trade-offs
- Bare surface requires cleanroom handling: Uncoated prime silicon forms a native oxide and is vulnerable to particulate and organic contamination; storage in dry nitrogen cabinets and edge-only handling with vacuum wands or PTFE/PEEK tweezers are mandatory.
- Wet processing needs EHS infrastructure: Native oxide removal and RCA cleaning require wet benches or exhaust fume hoods under institutional EHS and SDS protocols, adding facility and safety compliance overhead.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).