6-Inch N-Type Silicon Wafer 10-20 Ω·cm DSP ATOMFAIR®

Price range: $429.00 through $979.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 150 mm CZ N-type silicon wafer, 675 μm, 10–20 Ω·cm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•10–20 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Phosphorus-doped to 10–20 Ω·cm (~2×1014–4.5×1014 cm-3 electron density), this moderate-resistivity n-type substrate minimizes ionized-impurity scattering and junction capacitance, supporting MOS capacitor gate metrology, photodiode arrays, and minority-hole diffusion lifetime studies.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>) SEMI M1 (150 mm N<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (10–20 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type (100), 10-20 ohm-cm, 675 um, DSP (This Product) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type (10–20 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type <100> Standard SEMI M1 675 μm 150 mm N-type lithography substrate
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type <100> Double-side CMP polished N-type 150 mm wafer for bonding & IR
6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulates, corrosive vapors, and uncontrolled humidity must be minimized to prevent surface contamination and native oxide growth.

  • Cleanroom Cassette Storage: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination.
  • Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle transfer.
  • Native Oxide Awareness: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxy if an oxide-free interface is required.
  • Wet Processing Containment: Perform all wet-chemical processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety guidelines.

Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to photoresist spin coating or deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Exhaust fume hood or wet bench, O2 plasma descum system

  1. Inspect wafer cassette
    Inspect the cleanroom cassette for particulate contamination and verify that wafers are immobilized by edge contact only before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood or wet bench.
  4. Dry with nitrogen
    Dry the wafer surface with a filtered N2 blow-dry to remove residual solvent and water droplets.
  5. Apply mild O2 plasma descum
    Apply a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD deposition.
  6. Return wafer to nitrogen storage
    Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet to prevent recontamination.

What is the resistivity and dopant specification of this 6-inch N-type silicon wafer?

This wafer is Phosphorus-doped N-type monocrystalline silicon with a verified bulk resistivity of 10–20 Ω·cm, corresponding to an electron density of approximately 2×10^14–4.5×10^14 cm^-3. The moderate resistivity minimizes ionized-impurity scattering and junction capacitance, making it suitable for MOS capacitor gate metrology, photodiode arrays, and minority-hole diffusion lifetime studies. Resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.

Is this wafer compatible with double-side lithography and wafer bonding processes?

Yes. This is a double-side polished (DSP) wafer with CMP mirror finish on both surfaces at Ra < 0.5 nm, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The <100> crystal orientation with ± 0.5° tolerance also enables KOH/TMAH anisotropic etching and Bosch DRIE for MEMS and CMOS prototyping. The SEMI M1 standard 675 ± 25 μm thickness provides high flexural stiffness for automated 150 mm photolithography steppers and epitaxial susceptors.

How should these prime silicon wafers be stored and handled to maintain surface quality?

Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm CMP surfaces. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm); if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

The 6-inch prime CZ N-type <100> silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a versatile substrate for double-side lithography, MEMS, and CMOS prototyping, but its bare surface requires strict cleanroom handling and immediate native-oxide management to preserve interface quality.

Positive

  • Dual-Side CMP Enables Bonding: Double-side mirror-polished surfaces with Ra < 0.5 nm support direct fusion and anodic bonding, double-sided MEMS patterning, and through-wafer IR transmission without additional surface preparation.
  • Moderate Resistivity Reduces Losses: Phosphorus doping at 10–20 Ω·cm minimizes ionized-impurity scattering and junction capacitance, benefiting MOS capacitor metrology, photodiode arrays, and minority-carrier lifetime studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm native SiO2 layer in ambient air; wet-chemical removal or RCA cleaning must be performed in an exhaust fume hood or wet bench following institutional EHS protocols before metallization or epitaxy.
  • Cleanroom Handling Mandatory: To prevent particulate contamination and preserve surface quality, wafers must be stored in dry nitrogen cabinets and handled only with vacuum wands or PTFE/PEEK tweezers by the perimeter edge.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)