6-Inch N-Type Silicon Wafer 0.1-1.0 Ω·cm SSP ATOMFAIR®

Price range: $319.00 through $699.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-type silicon wafer, 150 mm, 675 μm, 0.1–1.0 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•0.1–1.0 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to 0.1–1.0 Ω·cm (~5×1015–8×1016 cm-3 electron concentration), this moderately low-resistivity n-type substrate bridges heavily doped electrode wafers and standard CMOS grades for epitaxial buffer templates, Schottky power diodes, and low-resistance MOS back gates.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.1–1.0 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>) SEMI M1 (150 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.1–1.0 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type (100), 0.1-1.0 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type (0.1–1.0 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type <100> Standard SEMI M1 675 μm 150 mm N-type lithography substrate
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type <100> Double-side CMP polished N-type 150 mm wafer for bonding & IR
6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in dry nitrogen or desiccator environments away from corrosive vapors and airborne organics.

  • Surface Contamination Sensitivity: The mirror-polished front surface (Ra < 0.5 nm) is sensitive to particulate deposition and organic contamination, requiring cleanroom handling with vacuum wands or PTFE/PEEK tweezers applied only at the wafer perimeter.
  • Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide layer of approximately 1–2 nm in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxial growth.
  • Storage Atmosphere Requirements: Unused wafers must remain sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination and particulate exposure.
  • Wet Processing Safety: All wet-chemical processing including RCA clean and native oxide removal must be performed inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.

Proper handling preserves the CMP mirror surface and prevents contamination during semiconductor processing. Sequential solvent cleaning and plasma descum prepare the wafer surface for photoresist coating or thin-film deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect wafer packaging
    Verify the cleanroom cassette seal is intact and inspect wafers for visible particulate or surface damage before opening.
  2. Handle by perimeter edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge to avoid contact with the polished surface.
  3. Perform solvent pre-cleaning
    Degrease wafers sequentially in acetone, electronic-grade isopropanol, and deionized water followed by nitrogen blow-drying.
  4. Apply plasma descum
    Subject the wafer to mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide if required
    Perform RCA standard clean or wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when native oxide removal is required before metallization or epitaxy.
  6. Store unused wafers properly
    Return unused wafers to the original cleanroom polypropylene cassette and store sealed within a dry nitrogen cabinet or desiccator.

What is the resistivity range and dopant of this 6-inch N-type silicon wafer?

This wafer is Phosphorus-doped N-type with a verified resistivity of 0.1–1.0 Ω·cm, corresponding to an electron concentration of approximately 5×10^15–8×10^16 cm^-3. The resistivity is measured by four-point probe (4PP) and documented on the lot-specific Certificate of Analysis. This moderately low-resistivity grade bridges heavily doped electrode wafers and standard CMOS grades.

Is this wafer compatible with KOH or TMAH anisotropic etching for MEMS fabrication?

Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, making it suitable for MEMS prototyping. The cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes. The primary flat is oriented along <110> ± 1° per SEMI M1, ensuring accurate mask alignment for etch-defined structures.

How should these prime silicon wafers be stored and handled to preserve surface quality?

Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the Ra < 0.5 nm polished front surface. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers sealed to minimize airborne organic contamination.

The 6-inch N-type <100> prime CZ silicon wafer with 0.1–1.0 Ω·cm resistivity and SSP finish provides a verified, SEMI M1-compliant substrate for epitaxy, power device prototyping, and in-house oxidation, though its bare surface and single-side polish demand strict cleanroom handling and limit use in bonding or IR applications.

Positive

  • CMP Mirror Surface for Thin-Film Growth: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for epitaxy, PVD, ALD, and high-resolution 150 mm stepper lithography.
  • SEMI M1 Dimensional Precision: 150.0 ± 0.3 mm diameter, 675 ± 25 μm thickness, and standard flats enable accurate registration on vacuum chucks, mask aligners, and FOUP/cassette carriers.

Trade-offs

  • Bare Surface Requires Immediate Processing: Native oxide (~1–2 nm) forms in air; wafers must be stored in dry nitrogen and processed promptly to avoid contamination or unintended oxide growth.
  • Single-Side Polish Limits Bonding: Fine-ground back surface is unsuitable for direct wafer bonding or backside alignment, restricting use in stacked or double-side processed devices.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.1-1.0 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)