| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.1–1.0 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Phosphorus-doped to 0.1–1.0 Ω·cm (~5×1015–8×1016 cm-3 electron concentration), this moderately low-resistivity n-type substrate bridges heavily doped electrode wafers and standard CMOS grades for epitaxial buffer templates, Schottky power diodes, and low-resistance MOS back gates.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.1–1.0 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>) | SEMI M1 (150 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.1–1.0 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), N-Type (100), 0.1-1.0 ohm-cm, 675 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, N-Type (0.1–1.0 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N-Type <100> | Standard SEMI M1 675 μm 150 mm N-type lithography substrate |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, N-Type <100> | Double-side CMP polished N-type 150 mm wafer for bonding & IR |
| 6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped epi & MOSFET substrate |
| 6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N+ Sb <100> | Minimal autodoping Sb-doped wafer for sharp high-T epitaxy |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require storage in a dry nitrogen cabinet or cleanroom desiccator to prevent particulate contamination and native oxide growth. Handling must be performed strictly by the wafer perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface damage.
- Environmental Storage: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Surface Contamination Control: Keep unused wafers in the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
- Handling Technique: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Native Oxide Awareness: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy if required.
Proper pre-cleaning and handling of prime silicon wafers preserves mirror-polished CMP cleanliness and ensures reproducible thin-film interfaces. The procedure involves solvent degreasing, plasma descum, and careful storage to prevent contamination.
Required Equipment: Cleanroom vacuum wands or PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Degrease Wafer
Degrease the wafer sequentially in acetone, electronic-grade isopropanol (IPA), and DI water. - Dry and Descum
Blow-dry the wafer with nitrogen and perform a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD. - Remove Native Oxide
Perform wet processing to remove native oxide or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Store Wafer
Store the wafer sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
What is the resistivity range of this 6-inch N-type silicon wafer and how does it affect device fabrication?
This wafer is Phosphorus-doped to a resistivity of 0.1–1.0 Ω·cm, corresponding to an electron concentration of approximately 5×10^15–8×10^16 cm^-3. This moderately low resistivity bridges heavily doped electrode wafers and standard CMOS grades, making it suitable for epitaxial buffer templates, Schottky power diodes, and low-resistance MOS back gates. The controlled doping supports ohmic contact formation and predictable C-V metrology.
Can this double-side polished silicon wafer be used for wafer bonding and through-wafer infrared applications?
Yes. The dual-side CMP finish (DSP, Ra < 0.5 nm) enables direct fusion and anodic bonding, double-sided MEMS patterning, and through-wafer infrared transmission. The 675 ± 25 μm thickness provides high flexural stiffness for automated handling, while the <100> crystal orientation supports KOH/TMAH anisotropic etching and Bosch DRIE processes.
How should these prime-grade silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 10 pcs or 25 pcs cassettes designed to immobilize edges and prevent surface contact during transit.
This 6-inch prime CZ N-type <100> silicon wafer with 0.1–1.0 Ω·cm phosphorus doping and dual-side CMP finish (Ra < 0.5 nm) is engineered for double-side lithography, wafer bonding, and epitaxial buffer templates, with SEMI M1 geometry ensuring compatibility across 150 mm cleanroom tooling. Its moderately low resistivity and bare prime surface support in-house oxidation and ohmic contact formation, but handling demands strict edge-only manipulation and dry nitrogen storage to preserve surface quality.
Positive
- Dual-Side CMP for Bonding and IR: Double-side mirror-polished surfaces with Ra < 0.5 nm enable direct fusion/anodic bonding, double-sided MEMS patterning, and through-wafer infrared transmission without additional surface preparation.
- Moderate N-Type Doping for Device Prototyping: Phosphorus-doped to 0.1–1.0 Ω·cm (~5×10^15–8×10^16 cm^-3), this substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial buffer layers, Schottky power diodes, and low-resistance MOS back gates.
Trade-offs
- Strict Cleanroom Handling Required: Bare prime silicon with no protective coating must be handled exclusively by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination and particle introduction.
- Native Oxide Formation in Ambient Air: An ambient ~1–2 nm native SiO2 film forms in air, requiring wet-chemical removal (e.g., RCA clean) inside an exhaust fume hood or wet bench before metallization or epitaxy, with strict adherence to institutional EHS and SDS protocols.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).