6-Inch N-Type Arsenic Silicon Wafer 0.001-0.005 Ω·cm ATOMFAIR®

Price range: $369.00 through $819.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 150 mm CZ N-type arsenic-doped silicon wafer, 0.001–0.005 Ω·cm, , 675 μm, DSP Ra<0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Arsenic (As)
<111>•0.001–0.005 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped 150 mm wafers the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-series-resistance vertical ohmic contacts.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Arsenic (As) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>) SEMI M1 (150 mm N<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type Arsenic (111), 0.001-0.005 ohm-cm, 675 um, DSP (This Product) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type (0.001–0.005 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type <100> Standard SEMI M1 675 μm 150 mm N-type lithography substrate
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type <100> Double-side CMP polished N-type 150 mm wafer for bonding & IR
6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade arsenic-doped silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in a dry nitrogen environment to minimize native oxide growth and airborne organic contamination.

  • Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled removal before metallization or epitaxy.
  • Storage Atmosphere: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the surface for photoresist spin coating or PVD/ALD deposition.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Verify the cleanroom protective cassette is sealed and free of particulate contamination before opening.
  2. Handle by perimeter edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge.
  3. Degrease sequentially
    Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Blow-dry the wafer surface with filtered nitrogen gas until no visible solvent residue remains.
  5. Perform plasma descum
    Apply a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD.
  6. Store unused wafers
    Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet.

Why choose arsenic-doped <111> silicon wafers over phosphorus-doped <100> for epitaxy and power devices?

Arsenic doping at 0.001–0.005 Ω·cm (N++) provides roughly an order of magnitude slower diffusion than phosphorus, which preserves abrupt doping profiles during high-temperature Si/SiGe epitaxy and power MOSFET/IGBT fabrication. The <111> orientation offers a densely packed three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies, unlike standard <100> silicon. Additionally, arsenic's covalent atomic radius closely matches silicon, minimizing lattice strain and misfit dislocations at ultra-high doping levels.

Can these 6-inch DSP wafers be used directly in automated 150 mm photolithography and epitaxy tools?

Yes. The 150.0 ± 0.3 mm diameter, 675 ± 25 μm thickness, and SEMI M1 flats (57.5 mm primary flat along <110>, 37.5 mm secondary flat) ensure compatibility with automated 150 mm steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. The double-side polished (DSP) finish with Ra < 0.5 nm supports double-sided lithography, IR transmission, and wafer bonding. The low TTV (< 3 μm) and bow/warp (< 25 μm) further ensure reliable vacuum chuck registration.

What are the storage and handling requirements to maintain the CMP surface quality of these prime silicon wafers?

Store wafers sealed in their original cleanroom protective cassettes inside a dry nitrogen cabinet or desiccator to prevent airborne organic contamination and native oxide growth beyond the ambient ~1–2 nm. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. For wet processing such as RCA clean or native oxide removal, perform strictly in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

The 6-inch N-type arsenic-doped <111> prime silicon wafer with DSP finish and 0.001–0.005 Ω·cm resistivity provides a low-strain, low-diffusivity substrate suited for Si/SiGe epitaxy, power device prototyping, and hexagonal heteroepitaxy. Its SEMI M1 geometry and sub-nanometer CMP surface support automated 150 mm tooling, but deployment requires cleanroom handling and wet-bench infrastructure to preserve the native-oxide-free interface.

Positive

  • Arsenic Doping Minimizes Lattice Strain: Arsenic's covalent radius closely matches silicon, reducing misfit dislocations at ultra-high doping, while its slow diffusion supports sharp doping profiles in Si/SiGe epitaxy and power MOSFET fabrication.
  • DSP Finish Enables Double-Side Processing: Dual-side CMP with Ra < 0.5 nm supports double-sided lithography, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.

Trade-offs

  • Native Oxide Requires Removal Before Critical Steps: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS protocols prior to metallization or epitaxy.
  • Cleanroom Storage and Handling Mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Arsenic (As)

Orientation

(111) ± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)