| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.001–0.005 Ω·cm |
Thickness: 625 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 625 ± 20 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The 625 ± 20 μm precision-tolerance thickness suits 150 mm MEMS micromachining, double-side alignment lithography, Bosch DRIE through-etching, and wafer bonding with tight cavity depth control. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 625 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 150 mm N<100>) | SEMI M1 (150 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), N-Type (100), 0.001-0.005 ohm-cm, 625 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 625 ± 20 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 625 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N-Type <100> | Standard SEMI M1 675 μm 150 mm N-type lithography substrate |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, N-Type <100> | Double-side CMP polished N-type 150 mm wafer for bonding & IR |
| 6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped epi & MOSFET substrate |
| 6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N+ Sb <100> | Minimal autodoping Sb-doped wafer for sharp high-T epitaxy |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only manipulation to preserve dual-side CMP surface integrity. Ambient native oxide growth and contamination sensitivity impose defined cleanroom handling and pre-processing constraints.
- Storage Atmosphere Constraint: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Manual Handling Constraint: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled removal before metallization or epitaxy.
- Wet-Processing Containment: Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
- Cassette Storage Constraint: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Sequential wet-chemical degreasing and plasma descum preserve mirror-polished CMP cleanliness prior to photoresist coating or thin-film deposition. Native oxide control and cassette storage maintain reproducible thin-film interfaces across cleanroom processing runs.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect cassette and wafer edges
Inspect the cleanroom cassette and wafer perimeter for particulate contamination before opening. - Transfer wafer by edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially in solvents
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry with nitrogen
Blow-dry the wafer with N2 until all solvent residue is removed from both surfaces. - Apply mild O2 plasma descum
Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide under containment
Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Return unused wafers to sealed storage
Return unused wafers to the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
Why does this 6-inch N-type silicon wafer use a 625 µm thickness instead of the standard 675 µm?
The 625 ± 20 µm thickness is specified to support 150 mm MEMS micromachining, double-side alignment lithography, Bosch DRIE through-etching, and wafer bonding with tight cavity depth control. This is thinner than the 675 ± 25 µm used by the standard 6-inch N-type <100> wafers in the same catalog, which are intended for general lithography and bonding. The tighter thickness tolerance of ± 20 µm, combined with TTV < 3 µm and bow/warp < 25 µm, helps maintain focus budget and etch-depth uniformity during through-wafer processing.
Can this 0.001–0.005 Ω·cm phosphorus-doped wafer be used for epitaxial growth without autodoping problems?
This wafer is degenerately doped with phosphorus to 0.001–0.005 Ω·cm (N++, ~10^19–10^20 cm^-3), which makes it suitable as a conductive substrate for III-V/GaN buffer heteroepitaxy and low-resistance backside ohmic contacts. However, phosphorus is a relatively fast diffuser compared with arsenic or antimony, so if your epitaxy process requires a sharp doping profile at high temperature, an arsenic-doped (0.001–0.005 Ω·cm) or antimony-doped (0.005–0.02 Ω·cm) 6-inch wafer from the same catalog may be more appropriate. The bare prime surface carries only a ~1–2 nm native oxide, so standard pre-epi cleaning such as RCA or in-situ H2 bake is required before growth.
What cleanroom handling and storage conditions are required to preserve the DSP Ra < 0.5 nm surface of this prime silicon wafer?
Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and unused wafers should remain sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. The dual-side CMP finish (Ra < 0.5 nm) and ≤ 10 particles/wafer specification are maintained only under these conditions; exposure to ambient air also grows a ~1–2 nm native SiO2 film that must be removed by RCA clean or wet processing in an exhaust fume hood before metallization or epitaxy. All wet-chemical processing must follow institutional EHS and SDS safety protocols.
The 6-inch N-type prime CZ silicon wafer with 0.001–0.005 Ω·cm resistivity and DSP finish provides a low-resistance, epi-ready substrate for ohmic contacts and MEMS prototyping, but its degenerate doping and bare surface demand careful handling to avoid contamination and require cleanroom infrastructure for wet processing.
Positive
- Degenerate doping enables ohmic contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (N++), the wafer provides metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates.
- Dual-side CMP finish supports bonding: Double-side polished surfaces with Ra < 0.5 nm enable double-sided lithography, through-wafer IR transmission, and direct fusion or anodic bonding with tight cavity depth control.
Trade-offs
- Bare surface requires immediate cleaning: The native oxide (~1–2 nm) and lack of protective coating necessitate solvent/plasma pre-cleaning and controlled storage in a dry nitrogen cabinet to prevent organic contamination.
- Wet processing needs cleanroom infrastructure: RCA cleans, native oxide removal, and anisotropic etching require an exhaust fume hood or wet bench with facility-approved EHS protocols, limiting use to equipped laboratories.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).