6-Inch Antimony-Doped Silicon Wafer 675μm ATOMFAIR®

Price range: $289.00 through $629.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-type Sb-doped Si wafer, ±0.5°, 0.005–0.02 Ω·cm, 150.0 ±0.3 mm, 675 ±25 μm, SSP Ra <0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Antimony (Sb)
<111>•0.005–0.02 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance 150 mm base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Antimony (Sb) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.005–0.02 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>) SEMI M1 (150 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type Antimony (111), 0.005-0.02 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type (0.005–0.02 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type <100> Standard SEMI M1 675 μm 150 mm N-type lithography substrate
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type <100> Double-side CMP polished N-type 150 mm wafer for bonding & IR
6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only manual contact to preserve the CMP mirror finish and prevent metallic contamination. Ambient exposure generates a 1–2 nm native oxide that must be removed under exhaust-ventilated wet-bench conditions prior to epitaxy or metallization.

  • Particulate and Organic Contamination Control: Store unused wafers sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or desiccator to minimize airborne organic and particulate contamination.
  • Edge-Only Manual Contact: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the Ra < 0.5 nm polished front surface.
  • Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be accounted for in any interface-sensitive epitaxy, ohmic contact, or C-V metrology workflow.
  • Wet-Chemical Processing Containment: Perform RCA standard cleans, native-oxide stripping, and other wet processing strictly inside an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
  • Corrosive Vapor and Thermal Exposure: Avoid storage near corrosive vapors and confirm that any elevated-temperature LPCVD or epitaxial step remains within the SEMI M1 675 ± 25 μm thickness and bow/warp tolerances.

This procedure covers cassette retrieval, edge-only transfer, solvent pre-cleaning, and native-oxide control prior to thin-film deposition or lithography. All wet-chemical steps must follow institutional EHS and SDS safety protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Retrieve wafer from sealed cassette
    Open the cleanroom protective cassette inside a controlled environment and lift the wafer by its perimeter edge using a vacuum wand or PTFE/PEEK tweezers.
  2. Inspect surface for particles
    Verify the polished front surface under bright-light or laser surface scan against the ≤ 10 particles per wafer acceptance criterion before processing.
  3. Degrease in solvent sequence
    Immerse the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residue prior to resist coating or deposition.
  4. Dry and descum
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum to eliminate residual organics before photoresist spin coating or PVD/ALD.
  5. Strip native oxide if required
    Perform RCA standard clean or native-oxide removal inside an exhaust fume hood or wet bench when an oxide-free interface is required for metallization or epitaxy.
  6. Return unused wafers to storage
    Seal remaining wafers inside the original cleanroom polypropylene cassette and place the cassette in a dry nitrogen cabinet or desiccator.

Why choose antimony-doped <111> silicon wafers over arsenic-doped <100> for epitaxy?

Antimony (Sb) doping provides exceptionally low vapor-phase out-diffusion (autodoping) during high-temperature LPCVD and epitaxial processes, which is critical for abrupt interfaces. The <111> orientation offers a densely packed three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies. In contrast, arsenic-doped <100> wafers, while having lower diffusivity, do not offer the same hexagonal symmetry for III-nitride growth.

Can these 6-inch antimony-doped wafers be used for GaN epitaxy?

Yes, the <111> crystal orientation and antimony doping make these wafers suitable for hexagonal epitaxy. The dense three-fold <111> lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, and the low autodoping of antimony ensures sharp interfaces during elevated-temperature processes. The mirror-polished front surface (Ra < 0.5 nm) ensures uniform nucleation for epitaxial growth.

How should I store and handle these prime silicon wafers to maintain surface quality?

Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the polished surface. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.

The 6-inch N-type antimony-doped <111> prime silicon wafer offers a low-resistivity, low-autodoping substrate with sub-nanometer surface polish, well-suited for epitaxy and power device prototyping. However, its <111> orientation and single-side polish impose specific constraints on bonding and etch processes that must be accounted for in cleanroom integration.

Positive

  • Low Autodoping Antimony Dopant: Antimony's low solid-state diffusivity and vapor-phase out-diffusion minimize autodoping during high-temperature LPCVD and epitaxial steps, enabling abrupt doping profiles for power MOSFETs and Schottky barriers.
  • Sub-Nanometer CMP Surface: The single-side polished front surface with Ra < 0.5 nm ensures uniform nucleation for epitaxy, ALD, and high-resolution lithography, supporting reproducible thin-film growth and device fabrication.

Trade-offs

  • <111> Orientation Etch Sensitivity: The <111> crystal plane exhibits slower wet alkaline etch kinetics and higher in-plane elastic modulus, which can complicate anisotropic etching and cleavage-based processes compared to <100> silicon.
  • Single-Side Polish Limits Bonding: The fine-ground back surface of this SSP wafer is not suitable for direct wafer bonding or backside alignment, restricting use in stacked or double-side processed device architectures.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Antimony (Sb)

Orientation

± 0.5°

Resistivity

0.005-0.02 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)