3-Inch N-Type Silicon Wafer 0.001-0.005 Ω·cm ATOMFAIR®

$299.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 76.2 mm, 380 μm, 0.001–0.005 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
3-Inch (76.2 ± 0.25 mm)
Primary Flat 22.22 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.001–0.005 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers very low bulk series resistance for low-resistance backside ohmic contacts, conductive bottom electrodes, III-V/GaN buffer heteroepitaxy, and high-current device testing.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 3-Inch Dimensional Precision

Standardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 76.2 ± 0.25 mm (3.0 Inch)
  • Primary Flat: 22.22 ± 3.17 mm along <110> ± 1°
  • Secondary Flat: 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 76.2 ± 0.25 mm (3-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 22.22 ± 3.17 mm SEMI M1 (76.2 mm)
Secondary Flat 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>) SEMI M1 (76.2 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (111), 0.001-0.005 ohm-cm, 380 um, SSP (This Product) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type (0.001–0.005 Ω·cm) SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools
3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Standard 76.2 mm P<100> bare lithography substrate
3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 3-Inch (76.2 mm) / DSP 380 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & wafer bonding
3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type <100> Phosphorus-doped N<100> substrate for Schottky & diode R&D
3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry an ambient native oxide of approximately 1–2 nm that must be removed or accounted for prior to metallization or epitaxy. Storage in a dry nitrogen cabinet within the original cassette is required to limit airborne organic contamination and particulate deposition.

  • Native Oxide Formation: Exposure to ambient air forms a 1–2 nm native SiO2 film that alters the surface chemistry before epitaxial or ohmic-contact processing.
  • Particulate and Organic Contamination: Unsealed storage permits airborne organics and particles to accumulate on the CMP mirror surface, degrading nucleation uniformity and lithographic resolution.
  • Edge-Contact Damage Risk: Direct contact with the polished face or ground back introduces scratches and micro-fractures that compromise device yield.
  • Wet-Chemical Processing Containment: RCA cleans and native-oxide removal must be performed in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.

Preserve the CMP mirror finish and reproducible thin-film interfaces by following a defined sequence of solvent cleaning, plasma descum, and controlled storage. Each step assumes a cleanroom environment with appropriate EHS oversight.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet

  1. Inspect cassette seal
    Verify the 25-wafer polypropylene cassette remains sealed and undamaged before opening in the cleanroom.
  2. Transfer wafer by edge
    Handle each wafer strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Immerse the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues.
  4. Dry and descum
    Blow-dry with nitrogen and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide if required
    Perform RCA standard clean or native-oxide removal in an exhaust fume hood or wet bench using facility-approved protocols.
  6. Store unused wafers
    Return unused wafers to the original cassette and store inside a dry nitrogen cabinet to minimize contamination.

Why choose a <111> N-type silicon wafer over <100> for GaN or AlN epitaxy?

The <111> orientation provides a hexagonal three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy, whereas <100> silicon does not. This wafer is oriented to <111> ± 0.5° and is degenerately phosphorus-doped to 0.001–0.005 Ω·cm, which also enables low-resistance backside ohmic contacts for GaN/AlN/SiC buffer growth. The higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics further differentiate it from standard <100> substrates.

Can this 3-inch N-type <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?

Yes, the wafer is bare prime silicon with only a thin ambient native oxide (~1–2 nm), so it can be loaded directly into a tube furnace for in-house dry/wet thermal SiO2 growth. However, for reproducible oxide thickness and interface quality, the source recommends solvent pre-cleaning (acetone, IPA, DI water) followed by N2 dry and mild O2 plasma descum before oxidation. Any wet-chemical processing must follow institutional EHS and SDS protocols.

What handling and storage precautions are required to maintain the Ra < 0.5 nm surface of this SSP wafer?

Handle the wafer strictly by its perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface. Store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. This preserves the CMP mirror finish (Ra < 0.5 nm) and prevents airborne organic contamination.

This 3-inch prime CZ N-type <111> silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with a sub-nanometer CMP front surface, making it well-suited for low-resistance ohmic contacts, III-nitride heteroepitaxy, and high-current device prototyping on standard 3-inch R&D tooling. Its bare, uncoated surface and SSP-only finish impose strict cleanroom handling and pre-cleaning discipline to preserve the polished interface.

Positive

  • Degenerate N++ Doping for Low Resistance: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), the substrate provides very low bulk series resistance for backside ohmic contacts, conductive bottom electrodes, and high-current device testing.
  • <111> Lattice for Hexagonal Epitaxy: The densely packed <111> (± 0.5°) orientation offers three-fold surface symmetry and slower wet alkaline etch kinetics than <100>, supporting GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and UHV surface reconstruction studies.
  • CMP Mirror Surface for Thin Films: Single-side CMP polishing achieves Ra < 0.5 nm, ensuring uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
  • 3-Inch Format Fits Standard Tooling: The 76.2 mm SEMI M1 geometry delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks.

Trade-offs

  • Bare Surface Requires Pre-Cleaning: The uncoated prime silicon forms a ~1–2 nm ambient native oxide in air; reproducible ohmic or epitaxial interfaces require solvent/plasma pre-cleaning and, where needed, RCA or native-oxide removal under exhaust fume hood or wet-bench protocols.
  • SSP Backside Limits Bonding Use: Only the front surface is CMP-polished (Ra < 0.5 nm); the fine-ground backside is unsuitable for double-side bonding or IR-optics applications that require DSP-grade rear-surface finish.
  • Strict Cleanroom Storage Required: Wafers must be stored sealed in the original 25-wafer cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors, and handled only by perimeter edge with vacuum wands or PTFE/PEEK tweezers.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

3-Inch (76.2 ± 0.25 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)