| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <111>•1–10 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Phosphorus to a standard 1–10 Ω·cm n-type semiconducting range, the wafer provides uniform majority-electron transport for Schottky rectifiers, n-channel CMOS/PMOS device R&D, dielectric C-V profiling, and cleanroom thin-film deposition.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>) | SEMI M1 (76.2 mm N<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (111), 1-10 ohm-cm, 380 um, SSP (This Product) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type (1–10 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only manipulation to preserve the CMP mirror finish. Ambient native oxide growth and surface contamination must be managed prior to any thin-film or lithographic processing.
- Cleanroom Storage Atmosphere: Store unused wafers sealed in the original polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Contact Protocol: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxy.
- Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.
Proper pre-cleaning and handling of prime silicon wafers ensures reproducible thin-film interfaces and prevents contamination during semiconductor processing. These steps cover solvent degreasing, native oxide control, and cassette storage.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator
- Degrease wafer surface
Degrease the wafer sequentially in acetone, electronic-grade isopropanol (IPA), and DI water. - Dry and descum
Blow-dry the wafer with nitrogen and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide
Perform RCA standard clean or wet processing inside an exhaust fume hood or wet bench to remove the native SiO2 film before metallization or epitaxy. - Store unused wafers
Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a <111> N-type silicon wafer over <100> for epitaxy or device R&D?
The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies, which are difficult on <100> silicon. It also exhibits a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100>. This makes it preferable for hexagonal epitaxy and discrete power/bipolar prototyping, whereas <100> remains the standard for mainstream CMOS lithography.
Can this 3-inch N-type <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?
Yes, the wafer is a bare prime silicon substrate with only a thin ambient native oxide (~1–2 nm), so it can be loaded directly into a tube furnace for in-house dry/wet thermal SiO2 growth. However, for reproducible interfaces before metallization or epitaxy, the source recommends solvent pre-cleaning (acetone, IPA, DI water), N2 blow-drying, and a mild O2 plasma descum. Any wet-chemical native oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
What handling and storage precautions are required to maintain the SSP Ra < 0.5 nm surface of this prime silicon wafer?
The single-side polished front surface has a measured roughness of Ra < 0.5 nm, so wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. Store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. This minimizes airborne organic contamination and preserves the CMP finish for subsequent lithography or thin-film deposition.
This 3-inch prime CZ N-type <111> silicon wafer with 1–10 Ω·cm phosphorus doping and SSP finish (Ra < 0.5 nm) is engineered for hexagonal epitaxy, III-nitride growth, and cleanroom thin-film R&D, offering SEMI M1 dimensional precision and a 25-wafer cassette format. Its <111> orientation and bare prime surface impose specific handling and pre-cleaning requirements, but the verified CoA and virgin substrate quality support reproducible device prototyping.
Positive
- Hexagonal <111> Lattice for Epitaxy: The densely packed <111> crystal plane provides three-fold surface symmetry and slower wet alkaline etch kinetics than <100>, directly supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
- Sub-Nanometer CMP Surface Finish: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating, enabling reproducible thin-film growth and lithography.
Trade-offs
- Native Oxide Requires Pre-Cleaning: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal via RCA or wet processing must be performed in an exhaust fume hood or wet bench using facility-approved protocols before metallization or epitaxy.
- Strict Cleanroom Handling Protocol: Wafers must be stored sealed in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).