3-Inch N-Type Silicon Wafer 0.01-0.1 Ω·cm ATOMFAIR®

$289.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 76.2 mm, 380 μm, 0.01–0.1 Ω·cm, SSP Ra<0.5 nm. SEMI M1 flats, 25 pcs cassette. Order now.

Diameter & Flat:
3-Inch (76.2 ± 0.25 mm)
Primary Flat 22.22 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.01–0.1 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+), the wafer combines low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 3-Inch Dimensional Precision

Standardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 76.2 ± 0.25 mm (3.0 Inch)
  • Primary Flat: 22.22 ± 3.17 mm along <110> ± 1°
  • Secondary Flat: 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 76.2 ± 0.25 mm (3-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 22.22 ± 3.17 mm SEMI M1 (76.2 mm)
Secondary Flat 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>) SEMI M1 (76.2 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (111), 0.01-0.1 ohm-cm, 380 um, SSP (This Product) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type (0.01–0.1 Ω·cm) SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools
3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Standard 76.2 mm P<100> bare lithography substrate
3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 3-Inch (76.2 mm) / DSP 380 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & wafer bonding
3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type <100> Phosphorus-doped N<100> substrate for Schottky & diode R&D
3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage and processing must occur under cleanroom conditions with strict exclusion of corrosive vapors and atmospheric moisture.

  • Native Oxide Formation: Exposure to ambient air forms a 1–2 nm native silicon dioxide film that must be removed by wet or plasma processing before epitaxy or metallization.
  • Particulate and Organic Contamination: Airborne particulates and organic vapors degrade the mirror-polished CMP surface and compromise thin-film nucleation uniformity.
  • Edge Handling Requirement: Direct contact with the polished face introduces scratches and metallic contamination, requiring perimeter-only handling with vacuum wands or PTFE/PEEK tweezers.
  • Dry Nitrogen Storage: Unused wafers must remain sealed in the original polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator.
  • Wet Chemical Safety: RCA cleans, HF native-oxide removal, and alkaline etching must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols.

Preserve CMP surface quality and reproducible thin-film interfaces by following sequential solvent cleaning, plasma descum, and controlled storage. All wet-chemical steps require facility-approved EHS and SDS compliance.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect cassette and wafer edges
    Verify the 25-wafer polypropylene cassette is intact and inspect wafer perimeters for edge chips before removing any substrate.
  2. Transfer wafer by perimeter only
    Lift the wafer strictly by its edge using a cleanroom vacuum wand or PTFE/PEEK tweezers, never contacting the polished front surface.
  3. Degrease in solvent sequence
    Immerse the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood to remove organic residues.
  4. Dry and descum
    Blow-dry the wafer with filtered N2 and apply a mild O2 plasma descum to eliminate residual organics prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide if required
    Perform RCA standard clean or HF native-oxide removal inside a wet bench under facility-approved EHS and SDS protocols before metallization or epitaxy.
  6. Return unused wafers to dry storage
    Seal remaining wafers in the original polypropylene cassette box and place inside a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a 0.01–0.1 Ω·cm N-type <111> silicon wafer instead of a standard 1–10 Ω·cm substrate for device prototyping?

The 0.01–0.1 Ω·cm phosphorus-doped (N+) range lowers substrate contact resistance for vertical diodes, ohmic contacts, and electrochemical electrodes while maintaining lower free-carrier optical loss than degenerately doped N++ wafers. Standard 1–10 Ω·cm wafers are intended for general lithography and isolation, not low-resistance current paths. The <111> orientation further provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon, which benefits III-nitride epitaxy and discrete power/bipolar R&D.

Can this 3-inch N-type <111> wafer be processed in standard 3-inch cleanroom tools without custom fixturing?

Yes. The 76.2 ± 0.25 mm diameter and SEMI M1 flats (22.22 ± 3.17 mm primary flat along <110> ± 1°, 11.18 ± 1.52 mm secondary flat at 45° ± 5° clockwise) are designed for standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. The format provides roughly 2.25× the usable patterning area of a 2-inch wafer while remaining compatible with existing 3-inch vacuum chucks and cleanroom cassettes.

What handling and storage precautions are required to preserve the Ra < 0.5 nm CMP surface of this bare prime silicon wafer?

Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and unused wafers should remain sealed in the original 25-wafer polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Bare prime silicon carries only a ~1–2 nm ambient native oxide, so any solvent/plasma pre-clean or RCA wet processing must follow institutional EHS and SDS protocols to avoid contaminating the mirror-polished front surface before PVD, ALD, or photoresist spin coating.

The 3-inch N-type <111> prime silicon wafer with 0.01–0.1 Ω·cm phosphorus doping and SSP finish offers a low-resistivity, hexagonal-symmetry substrate suited for III-nitride epitaxy, vertical diode prototyping, and electrochemical electrodes. Its 380 µm thickness and SEMI M1 flats ensure compatibility with standard 3-inch cleanroom tools, though the single-side polish and bare surface require careful native-oxide management and edge-only handling.

Positive

  • Low-resistivity N+ doping: Phosphorus-doped to 0.01–0.1 Ω·cm, the substrate provides low contact resistance for vertical diodes and electrochemical electrodes while maintaining lower free-carrier optical loss than degenerately doped N++ wafers.
  • <111> orientation for hexagonal epitaxy: The <111> ± 0.5° crystal plane offers three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native oxide requires removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure reproducible ohmic interfaces.
  • Edge-only handling mandatory: The mirror-polished front surface (Ra < 0.5 nm) is vulnerable to particulate contamination; wafers must be handled strictly by the perimeter using cleanroom vacuum wands or PTFE/PEEK tweezers and stored in a dry nitrogen cabinet.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

3-Inch (76.2 ± 0.25 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)