| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•100–1000 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | None (SEMI M1 standard for 50.8 mm P-type <111>) | SEMI M1 (50.8 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 100-1000 ohm-cm, 275 um, SSP (This Product) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type (100–1000 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate contamination, airborne organics, and corrosive vapors. Storage must remain sealed in a dry nitrogen cabinet or cleanroom desiccator, with handling restricted to perimeter edges using cleanroom-compatible tools.
- Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1–2 nm in air, which must be removed by wet processing or RCA clean before metallization or epitaxy.
- Particulate and Organic Contamination Control: Unused wafers must remain sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
- Edge-Only Handling Requirement: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and damage.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, with native oxide removal or RCA standard clean performed inside an exhaust fume hood or wet bench.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces by following sequential solvent cleaning, plasma descum, and controlled storage. All steps require cleanroom-compatible tools and adherence to institutional safety protocols.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer cassette
Inspect the sealed 25-wafer polypropylene cassette for integrity and confirm the lot-specific Certificate of Analysis before opening. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid surface contact. - Degrease sequentially
Degrease whole wafers or diced dies sequentially in acetone, electronic-grade isopropanol, and deionized water. - Dry and descum
Dry the wafer with nitrogen blow-drying and apply a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide if required
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when required before metallization or epitaxy. - Store unused wafers
Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a high-resistivity 100–1000 Ω·cm P-type <111> silicon wafer instead of a standard 1–10 Ω·cm wafer?
The 100–1000 Ω·cm Boron-doped resistivity substantially suppresses free-carrier conductive loss and parasitic capacitance, which is why this substrate is specified for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. Standard 1–10 Ω·cm wafers are optimized for conventional device fabrication but introduce higher dielectric loss at high frequencies. This wafer is also grown along the <111> (± 0.5°) plane, providing hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon.
Can this 2-inch P-type <111> silicon wafer be used for GaN or AlN epitaxy?
Yes. The densely packed <111> crystal orientation supports III-nitride/hexagonal epitaxy, including GaN, AlN, and SiC, as well as UHV surface reconstruction studies and discrete power/bipolar R&D. The single-side polished front surface with Ra < 0.5 nm ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating. The wafer is bare prime silicon with only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation or epitaxial growth.
How should these 2-inch prime silicon wafers be stored and handled to preserve surface quality?
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack) that immobilizes edges and prevents surface contact during transit. Store the sealed cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm CMP surface.
The 2-inch P-type <111> CZ silicon wafer at 100–1000 Ω·cm combines high bulk resistivity with a sub-nanometer CMP finish, making it a strong substrate for RF/microwave loss reduction, hexagonal III-nitride epitaxy, and UHV surface studies. Its 275 μm thickness and SEMI M1 flats fit standard 2-inch R&D chambers, but the bare native oxide and edge-handling requirements demand cleanroom discipline and wet-bench infrastructure.
Positive
- High-Resistivity Suppresses Conductive Loss: Boron doping at 100–1000 Ω·cm reduces free-carrier absorption and parasitic capacitance, directly benefiting RF/microwave coplanar waveguides, THz/IR windows, and photodetector isolation.
- <111> Lattice for Hexagonal Epitaxy: The densely packed <111> plane provides three-fold surface symmetry and slower alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction experiments.
Trade-offs
- Native Oxide Requires Wet Processing: Bare prime silicon carries a 1–2 nm ambient SiO2 layer that must be removed via RCA or wet etch inside an exhaust fume hood or wet bench before metallization or epitaxy, adding facility and EHS overhead.
- Edge-Only Handling Mandate: The mirror-polished SSP front surface is vulnerable to particulate and organic contamination; wafers must be handled strictly by the perimeter using vacuum wands or PTFE/PEEK tweezers and stored in a dry nitrogen cabinet.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).