2-Inch P-Type Silicon Wafer 1-10 Ω·cm SSP ATOMFAIR®

$259.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type/Boron silicon wafer, 50.8 mm, 275 μm, 1–10 Ω·cm, SSP Ra<0.5 nm. SEMI M1 flats, 25 pcs cassette. Order now.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•1–10 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 50.8 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat None (SEMI M1 standard for 50.8 mm P-type <111>) SEMI M1 (50.8 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 1-10 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type (1–10 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch N-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <111> N-type Phosphorus <111> wafer (45° secondary flat)

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage and handling must preserve the CMP mirror finish and prevent surface degradation prior to processing.

  • Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1–2 nm in air, which must be removed before metallization or epitaxial growth.
  • Particulate and Organic Contamination Control: Unused wafers must remain sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic and particulate contamination.
  • Edge-Only Handling Requirement: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contact with the polished front surface.
  • Corrosive Vapor Exposure: Storage away from corrosive vapors and particulate dust is required to prevent surface chemistry alteration and defect introduction.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.

Proper pre-cleaning and handling preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent degreasing followed by plasma descum prepares the surface for photoresist spin coating or PVD/ALD deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer Edges
    Inspect the sealed 25-wafer cleanroom cassette for integrity and verify wafer edges are immobilized before opening.
  2. Transfer Wafer by Perimeter Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood or wet bench.
  4. Dry with Nitrogen
    Blow-dry the wafer with nitrogen gas to remove residual solvent and water from the polished surface.
  5. Apply Mild O2 Plasma Descum
    Apply a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove Native Oxide if Required
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols where metallization or epitaxy requires it.
  7. Store Unused Wafers in Nitrogen Cabinet
    Store unused wafers sealed inside the original polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> oriented silicon wafer over <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed crystal plane with hexagonal three-fold surface symmetry, a higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon. These properties make it preferable for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. In contrast, <100> is typically chosen for standard CMOS lithography where faster etch rates and different surface chemistry are advantageous.

What is the native oxide thickness on this bare prime silicon wafer and how does it affect processing?

Bare prime silicon carries only a thin ambient native oxide of approximately 1–2 nm. This native oxide allows direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth without prior removal. However, for applications requiring ohmic contacts or epitaxy, the native oxide must be removed using RCA standard clean or wet processing inside an exhaust fume hood or wet bench, following institutional EHS and SDS safety protocols.

How should 2-inch prime silicon wafers be stored and handled to maintain surface quality?

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25BX) that immobilizes edges and prevents surface contact. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the mirror-polished front surface (Ra < 0.5 nm) and prevent contamination.

The 2-inch P-type <111> prime CZ silicon wafer with 1–10 Ω·cm boron doping and Ra < 0.5 nm SSP finish provides a well-characterized substrate for hexagonal epitaxy, thin-film deposition, and device prototyping in research-scale chambers. Its <111> orientation and SEMI M1 dimensional precision support reproducible processing, though users must manage native oxide formation and strict cleanroom handling to preserve surface quality.

Positive

  • Sub-nanometer CMP surface finish: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, and high-resolution photoresist spin coating, supporting reproducible thin-film growth and lithography.
  • <111> orientation for hexagonal epitaxy: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies, with slower wet alkaline etch kinetics than <100> silicon.

Trade-offs

  • Native oxide requires removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet processing or RCA clean is necessary before metallization or epitaxy, requiring exhaust fume hood or wet bench facilities.
  • Strict cleanroom handling required: Wafers must be stored in dry nitrogen cabinets and handled by perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and preserve surface quality.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)