2-Inch N-Type Silicon Wafer 100-1000 Ω·cm SSP ATOMFAIR®

$289.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 2-inch (50.8 mm) CZ N-type silicon wafer, 275 ± 25 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•100–1000 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat Located 180° ± 5° from primary flat (SEMI M1 50.8 mm N<100>) SEMI M1 (50.8 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (100), 100-1000 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin monocrystalline silicon wafers require particulate-controlled storage and edge-only handling to preserve the CMP mirror finish and prevent surface contamination. Environmental exposure to airborne organics, corrosive vapors, and uncontrolled humidity degrades the native oxide state and compromises downstream lithography and thin-film nucleation.

  • Cleanroom Cassette Storage: Store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination.
  • Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy where oxide removal is critical.
  • Corrosive Vapor Exclusion: Keep wafers away from particulate dust and corrosive vapors that can degrade the CMP surface and alter surface-state properties.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs by following sequential solvent cleaning, plasma descum, and controlled storage procedures. All wet-chemical processing must follow institutional EHS and SDS safety protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system

  1. Inspect wafer cassette
    Inspect the sealed 25-wafer cleanroom cassette for edge immobilization integrity and surface contact damage before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic surface contamination.
  4. Blow-dry with nitrogen
    Blow-dry the wafer with N2 to remove residual solvent before further processing.
  5. Apply mild O2 plasma descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition to ensure surface cleanliness.
  6. Perform wet processing in fume hood
    Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  7. Return wafer to nitrogen storage
    Return unused wafers to the original polypropylene cassette and store within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a 100–1000 Ω·cm high-resistivity n-type silicon wafer instead of a standard 1–10 Ω·cm substrate?

The 100–1000 Ω·cm phosphorus-doped CZ substrate is specified to suppress conductive substrate coupling and parasitic RF loss, making it suited to RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors. Standard 1–10 Ω·cm wafers are intended for more conventional device and lithography work, so the high-resistivity grade is the appropriate choice when substrate loss and coupling must be minimized. The trade-off is that the lighter doping provides a less conductive base, which must be accounted for in contact and device designs.

Can this 2-inch N-type <100> SSP wafer be used for KOH or TMAH anisotropic wet etching and DRIE?

Yes. The wafer is sliced along the <100> (± 0.5°) plane, which supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions as well as Bosch deep reactive ion etching (DRIE) for MEMS micromachining. The cubic <100> surface also provides four-fold rotational symmetry with clean perpendicular cleaving along <110> planes. Note that the back surface is fine-ground rather than polished, so backside lithography or bonding should not be assumed without further surface preparation.

How should these bare prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm polished surface?

Keep unused wafers sealed in the original 25-wafer polypropylene cleanroom cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the CMP-polished front face (Ra < 0.5 nm). Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any wet-chemical cleaning or native-oxide removal must follow institutional EHS and SDS protocols in an exhaust fume hood or wet bench.

The 2-inch prime CZ N-type <100> silicon wafer with 100–1000 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is a high-resistivity substrate suited for RF/microwave planar circuits, IR/THz windows, and low-noise MEMS, but its bare surface requires immediate native-oxide management and cleanroom handling to preserve interface quality.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this CZ wafer suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar circuits and low-noise MEMS sensors.
  • Precision <100> Orientation and Flats: The <100> (± 0.5°) crystal orientation with SEMI M1 flats enables predictable anisotropic KOH/TMAH V-groove etching and accurate registration on vacuum chucks and mask aligners.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench before metallization or epitaxy to ensure ohmic interfaces.
  • Cleanroom Storage and Handling Mandate: Wafers must be stored sealed in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge with cleanroom vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)