| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Antimony (Sb) <111>•0.005–0.02 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance 200 mm base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Antimony (Sb) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.005–0.02 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Antimony (111), 0.005-0.02 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (0.005–0.02 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade antimony-doped silicon substrates require particulate-controlled storage and edge-only manipulation to preserve CMP surface integrity. Ambient native oxide growth and atmospheric contamination must be managed prior to any thermal or epitaxial processing.
- Cleanroom Storage Atmosphere: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Manipulation: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Native Oxide Control: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air that must be removed via RCA standard clean or wet processing before metallization or epitaxy.
- Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or automated wet bench.
- Cassette Immobilization: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.
Sequential solvent cleaning, native oxide management, and controlled storage preserve CMP surface quality on prime antimony-doped silicon substrates. Each step must be performed under institutional EHS-compliant cleanroom conditions.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator, 200 mm cleanroom polypropylene cassette or FOUP carrier
- Inspect Cassette and Wafer Edges
Inspect the sealed cassette and wafer edges for particulate contamination or mechanical damage before opening in the cleanroom. - Transfer Wafer by Perimeter Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge. - Degrease in Solvent Sequence
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water or perform a megasonic SC-1 clean. - Dry and Descum Surface
Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide if Required
Perform RCA standard clean or wet oxide removal inside an exhaust fume hood or automated wet bench when metallization or epitaxy demands an oxide-free interface. - Return Unused Wafers to Sealed Storage
Return unused wafers to the original cleanroom cassette or FOUP carrier and store inside a dry nitrogen cabinet.
Why choose antimony-doped <111> silicon over phosphorus-doped <100> for a 200 mm epitaxy substrate?
Antimony (Sb) is selected when you need a heavily doped N+ base (0.005–0.02 Ω·cm, ~1.5×10^18–1.2×10^19 cm^-3) with minimal dopant movement during high-temperature processing. Sb exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (autodoping) during LPCVD and epitaxial steps, which preserves abrupt doping profiles. The <111> orientation adds a densely packed three-fold surface symmetry with slower wet alkaline etch kinetics than <100>, making it suitable for 200 mm GaN-on-Si/III-nitride epitaxy and discrete power/bipolar R&D.
Can this 8-inch N-type antimony wafer be used directly in a 200 mm FOUP-compatible cluster tool without a carrier wafer?
Yes. The wafer meets SEMI M1 200 mm geometry with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a single SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°). This thickness provides high flexural stiffness for automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The bare prime surface carries only a thin ambient native oxide (~1–2 nm), so no carrier wafer is required for standard handling.
What cleanroom storage and handling protocol is required to maintain the DSP surface of this prime antimony-doped wafer?
Store wafers sealed inside the original 200 mm cleanroom protective cassette or FOUP within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. For pre-cleaning, use electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum before photoresist spin coating or PVD/ALD.
The 8-inch prime CZ antimony-doped <111> silicon wafer delivers a low-resistivity N+ base with suppressed autodoping for epitaxy and power-device R&D, while its DSP finish and SEMI M1 geometry support automated 200 mm tooling. Deployment requires cleanroom handling and wet-bench infrastructure to preserve the CMP surface and manage native oxide before critical interfaces.
Positive
- Antimony doping suppresses autodoping: Antimony's very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion minimize autodoping during elevated-temperature LPCVD and epitaxial processes, supporting abrupt silicon epitaxy and buried-layer R&D.
- DSP finish enables double-side processing: Dual-side CMP mirror polish with Ra < 0.5 nm and TTV < 3 μm supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion or anodic bonding.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; native oxide removal or RCA standard clean must be performed in an exhaust fume hood or automated wet bench using facility-approved protocols before metallization or epitaxy.
- Cleanroom handling mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).