8-Inch N-Type Antimony Silicon Wafer 725μm ATOMFAIR®

Price range: $299.00 through $1,199.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ 200mm N-type Sb-doped Si wafer, , 0.005–0.02 Ω·cm, 725 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 V-notch. In stock.

Diameter & Notch:
8-Inch (200.0 ± 0.2 mm)
SEMI V-Notch <110>
Substrate & Dopant:
CZ N-Type / Antimony (Sb)
<111>•0.005–0.02 Ω·cm
Thickness:
725 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance 200 mm base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.

8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 8-Inch Notch & Precision

Standardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.

  • Diameter: 200.0 ± 0.2 mm (8.0 Inch)
  • Primary Fiducial: SEMI V-Notch along <110> ± 1° (Depth 1.0 +0.25/-0.00 mm, 90°)
  • Secondary Fiducial: None (SEMI M1 200 mm notch standard)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Antimony (Sb) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.005–0.02 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 200.0 ± 0.2 mm (8-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 725 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Fiducial (Notch) SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) SEMI M1 (200 mm)
Secondary Flat / Notch None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) SEMI M1 / Lot Laser ID
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes 200 mm Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
  • Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
  • 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
  • In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 8-Inch (200 mm), N-Type Antimony (111), 0.005-0.02 ohm-cm, 725 um, SSP (This Product) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type (0.005–0.02 Ω·cm) SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, P-Type <100> Standard SEMI M1 200 mm notch CMOS & lithography substrate
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) 8-Inch (200 mm) / DSP 725 ± 25 μm, P-Type <100> Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics
8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type <100> Phosphorus-doped 200 mm wafer for power & CMOS R&D
8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped 200 mm epi substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require cleanroom-compatible storage to prevent particulate and organic contamination. Antimony-doped <111> wafers must be protected from corrosive vapors and handled only by perimeter edges or robotic end-effectors.

  • Cleanroom Storage Atmosphere: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling: Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for native oxide removal before metallization or epitaxy.
  • Wet Processing Containment: Perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
  • Cassette Immobilization: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, native oxide control, and proper cassette storage to maintain prime-grade surface quality.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect cassette packaging
    Verify the 200 mm cleanroom protective cassette is intact and wafers are immobilized by edge contact before opening.
  2. Transfer with edge-only contact
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease sequentially
    Degrease wafers sequentially in electronic-grade acetone, isopropanol, and DI water or perform megasonic/SC-1 clean.
  4. Dry and descum
    Blow-dry with N2 and apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide under containment
    Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
  6. Store unused wafers sealed
    Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet.

Why choose antimony-doped <111> silicon wafers over phosphorus-doped <100> for epitaxy and power device R&D?

Antimony (Sb) offers very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (autodoping) during elevated-temperature LPCVD and epitaxial processes, which preserves abrupt doping profiles at the epi/substrate interface. This wafer is doped to 0.005–0.02 Ω·cm (N+, ~1.5×10^18–1.2×10^19 cm^-3) along the <111> plane, whose densely packed three-fold symmetry supports 200 mm GaN-on-Si/AlN heteroepitaxy and discrete power/bipolar R&D. In contrast, phosphorus-doped <100> wafers are typically used for standard CMOS and power R&D where autodoping control is less critical.

Can this 8-inch N-type antimony <111> wafer be used directly in a 200 mm CMOS or epitaxy cluster tool without additional surface preparation?

Yes, the wafer is a prime-grade, virgin substrate with SEMI M1 200 mm dimensions (200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness) and a SEMI V-notch along <110> ± 1°, making it compatible with automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The front surface is single-side polished (SSP) with Ra < 0.5 nm and TTV < 5 μm, suitable for uniform nucleation in epitaxy, PVD/CVD, ALD, and stepper lithography. However, bare prime silicon carries a native oxide (~1–2 nm), so if your process requires an oxide-free interface, an in-house RCA clean or HF dip must be performed prior to deposition.

What are the storage and handling requirements to maintain the surface quality of these antimony-doped silicon wafers?

Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent surface contamination and native oxide growth beyond the ambient ~1–2 nm. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. The wafers are shipped in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges and prevent surface contact during transit.

This 200 mm prime CZ silicon wafer combines antimony doping at 0.005–0.02 Ω·cm with a <111> orientation and SSP finish (Ra < 0.5 nm), making it a strong substrate candidate for GaN-on-Si heteroepitaxy, abrupt epi layers, and power-device R&D where autodoping control and surface planarity are critical. Its SEMI M1 geometry and 725 μm thickness align with automated 200 mm FOUP, lithography, and CMP tooling, though successful use depends on cleanroom-grade handling and wet-bench infrastructure for native-oxide removal.

Positive

  • Low Autodoping Antimony Dopant: Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion during elevated-temperature LPCVD and epitaxial processes, supporting abrupt doping profiles in epitaxial and buried-layer structures.
  • SEMI M1 200 mm Tool Compatibility: The 200.0 ± 0.2 mm diameter, SEMI V-notch fiducial, and 725 ± 25 μm thickness conform to SEMI M1, enabling direct loading into automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.

Trade-offs

  • Native Oxide Requires Wet Processing: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal before metallization or epitaxy requires wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
  • Cleanroom Storage and Handling Mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handled strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

5 pcs, 10 pcs, 25 pcs

Diameter

8-Inch (200.0 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Antimony (Sb)

Orientation

± 0.5°

Resistivity

0.005-0.02 Ω·cm

Thickness

725 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)